Ceramic Fiber Blanket & Board
A1: Yes, our products are exported to Europe. Like RHI, Calderys and Intocast are all our customers. We export firebrick, magnesia chrome brick and insulation material to them.
A2: Yes, please refer to the FCL quantity below.
CF blanket |
Packaging Qty(rolls) |
|||||
Temp |
B/D |
Size (mm) |
U.W. (Kg/pc) |
Rolls /Pallet |
20 GP |
40 HQ |
1260 |
96 |
14400x610x13 |
10.96 |
16/20/pallet |
160 |
420 |
1260 |
96 |
7200x610x19 |
8.01 |
16/20/pallet |
160 |
420 |
1260 |
96 |
7200x610x25 |
10.54 |
16/20/pallet |
160 |
420 |
1260 |
96 |
3600x610x50 |
10.54 |
16/20/pallet |
160 |
420 |
1260 |
128 |
14400x610x13 |
14.62 |
16/20/pallet |
160 |
420 |
1260 |
128 |
7200x610x19 |
10.68 |
16/20/pallet |
160 |
420 |
1260 |
128 |
7200x610x25 |
14.05 |
16/20/pallet |
160 |
420 |
1260 |
128 |
3600x610x50 |
14.05 |
16/20/pallet |
160 |
420 |
1400 |
128 |
14400x610x13 |
14.62 |
16/20/pallet |
160 |
420 |
1400 |
128 |
7200x610x19 |
10.68 |
16/20/pallet |
160 |
420 |
1400 |
128 |
7200x610x25 |
14.05 |
16/20/pallet |
160 |
420 |
1400 |
128 |
3600x610x50 |
14.05 |
16/20/pallet |
160 |
420 |
A3: Yes, please refer to the FCL quantity below.
CF board |
Packaging Qty(pcs) |
|||||
Temp |
B/D |
Size (mm) |
U.W. (Kg/pc) |
Pieces /Pallet |
20 GP |
40 HQ |
1260 |
300 |
1000x500x15 |
2.25 |
300/354/pallet |
3000 |
8496 |
1260 |
300 |
1000x500x30 |
4.5 |
150/176/pallet |
1500 |
4224 |
1260 |
300 |
1000x500x40 |
6 |
112/132/pallet |
1120 |
3168 |
1260 |
300 |
1000x500x50 |
7.5 |
90/104/pallet |
900 |
2496 |
1260 |
300 |
1000x500x60 |
9 |
74/88/pallet |
740 |
2112 |
1260 |
300 |
1000x500x70 |
10.5 |
64/74/pallet |
640 |
1776 |
Ceramic Fiber Rope
A1: For shape normal we have two types: round rope and square rope.
For material normal we have two types: rope with stainless steel wire reinforcement and rope with fiberglass reinforcement.
A2:1.Stainless steel wire reinforcement,working temp is about 1050℃-1100℃,because the highest working temp of Stainless steel is around 1050℃.
2.Fiberglass reinforcement,working temp can arrive 550℃-650℃,because the highest working temp of Fiberglass is around 600℃.
A3: Normally the packing is plastic protective film+woven bag. If requested we can customize hard card carton for customers with required Logo, charges separate calculate according actual situation.
Ceramic Fiber Rope
A1: The standard size of ceramic fiber paper thickness is 0.5-10MM, and the standard size of width is 610MM/1220MM. There is no limit to the length.But if it is packed in a carton, it is recommended not to exceed 7.32KG (the density of fiber paper is 200kg/m3).
For example:12M*610MM*5MM/6M*610MM*10MM
A2: Ceramic fiber paper packaging: ceramic fiber paper packaging is generally carton packaging,The standard carton size of roll ceramic fiber paper: 320*320*620MM
Pieces of ceramic fiber paper cartons are customized according to the size specified by the customer.
A3: The surface of ceramic fiber paper has some waterproof effect, but it should not be soaked in water for a long time.The water-proof effect of soluble fiber paper is better than fiber paper.
It is recommended to test according to the actual use environment (free samples can be provided)