Alumina Silica Brick

Along with the "Client-Oriented" enterprise philosophy, a rigorous high-quality control process, superior production products along with a robust R&D group, we constantly deliver premium quality products, exceptional solutions and aggressive costs for Alumina Silica Brick, Precast Concrete Retaining Wall Systems, Monolithic Castable Refractory, Lightweight Castable Refractory, Welcome you to be a part of us alongside one another to create your company easier. We're normally your finest partner when you want to have your own organization. Attaining consumer satisfaction is our company's purpose without end. We will make wonderful endeavours to produce new and top-quality merchandise, satisfy your exclusive requirements and supply you with pre-sale, on-sale and after-sale services for Alumina Silica Brick, Our Company has professional engineers and technical staff to answer your questions about maintenance problems, some common failure. Our product quality assurance, price concessions, any questions about the products, Please feel free to contact us.


  • Factory Supply Alumina Silica Brick - Ladle Shroud – Topower

    Factory Supply Alumina Silica Brick - Ladle Shroud – Topower

    Description Ladle shroud also known as the protective sleeve, is mainly used between the ladle and the tundish. It is an important part of the connection between the ladle and the tundish. The lower part of the upper connecting ladle is connected with the water outlet of the sliding nozzle device, and the lower end extends into the tundish. It prevents the molten steel entering the tundish from the ladle from being re-oxidized and splashed; protects the molten steel from secondary oxidat...
  • Special Price for Insulation Bricks - Fused Cast AZS Block – Topower

    Special Price for Insulation Bricks - Fused Cast AZS Block – Topower

    Description Fused cast AZS block manufacturing process mixes selected zircon sand and industrial alumina powder at a ratio of 1:1, plus a small amount of Na2O (added in the form of sodium carbonate), B2O3 (added in the form of boric acid or borax) flux, and mix well After being melted at 1800~1900℃, it can be cast to form a fused-cast brick containing 33% ZrO2. On this basis, using partially desiliconized zircon sand as raw material, fused-cast bricks containing 36% to 41% ZrO2 can be pr...
  • Best quality Alumina Bubble Brick - Zircon Nozzle – Topower

    Best quality Alumina Bubble Brick - Zircon Nozzle – Topower

    Description Zircon nozzle is made of high-temperature refractory materials, and can also be used to connect the process, which plays a great role in controlling the flow of molten steel. The zirconium sizing nozzle has good shock and heat resistance, very high stability, and has a certain anti-corrosion function. The zirconium sizing nozzle can effectively ensure the stability of molten steel inflow and ensure the normal processing of the processing procedure. The zirconium sizing nozzle...
  • Good Wholesale Vendors Brick Oven Insulation - Magnesia Chrome Brick – Topower

    Good Wholesale Vendors Brick Oven Insulation - Magnesia Chrome Brick – Topower

    Description Magnesia chrome brick is made of high-grade magnesite clinker and chromium oxide as raw materials, through high-pressure molding and high-temperature firing, the maximum allowable ambient temperature is 1700°C. Magnesia chrome brick has good heat peeling resistance, high alkali corrosion resistance and high thermal shock resistance characteristics, and it is environmentally friendly and has a long service life. Features High strength and high refractoriness / High alkal...
  • Good Quality Shape Refractory - Corundum Brick – Topower

    Good Quality Shape Refractory - Corundum Brick – Topower

    Description The alumina content of corundum brick is more than 90% and the main crystal phase is corundum. It has high compressive strength at room temperature (up to 340MPa), high load softening start temperature (more than 1700℃), good chemical stability, and strong resistance to acidic or alkaline slag, metal and molten glass, etc. Resistance. Thermal shock stability is related to its structure, and the corrosion resistance of dense products is good. There are two types of sintered c...
  • Excellent quality Ladle Shroud - Magnesia Hercynite Brick – Topower

    Excellent quality Ladle Shroud - Magnesia Hercynite Brick – Topower

    Description Magnesia hercynite bricks have the advantages of chromium-free environmental protection, good thermal shock stability, good kiln skin hanging ability, good corrosion resistance, low thermal expansion and low thermal conductivity, and better structural flexibility. In practical applications, the brick has a service life of more than 1 year, the kiln skin is hung quickly in the firing zone, the thickness of the kiln skin is uniform and stable, the refractory bricks have no larg...
  • Super Lowest Price Refractory Insulation Bricks - Alumina bubble brick – Topower

    Super Lowest Price Refractory Insulation Bricks - Alumina bubble brick – Topower

    Description Alumina bubble brick is one of the ultra-high temperature material energy-saving insulation materials. It uses alumina hollow spheres as the main raw material and combines with other binders to fire alumina hollow spheres in a high temperature furnace at 1750℃. Alumina bubble brick has the characteristics of low thermal conductivity, good heat preservation, high compressive strength, and can work at temperatures below 1800°C. It has excellent heat resistance and heat insulati...
  • Manufacturer for Special Alumina Brick - Corundum Brick – Topower

    Manufacturer for Special Alumina Brick - Corundum Brick – Topower

    Description The alumina content of corundum brick is more than 90% and the main crystal phase is corundum. It has high compressive strength at room temperature (up to 340MPa), high load softening start temperature (more than 1700℃), good chemical stability, and strong resistance to acidic or alkaline slag, metal and molten glass, etc. Resistance. Thermal shock stability is related to its structure, and the corrosion resistance of dense products is good. There are two types of sintered c...
  • New Fashion Design for Perlite Fire Brick - Porous Plug and Seat Well Block – Topower

    New Fashion Design for Perlite Fire Brick - Porous Plug and Seat Well Block – Topower

    Description Seat well block is made of corundum, chrome corundum and corundum spinel. It is the supporting product of separate and integral breathable brick, which has high thermal strength, good thermal stability, scour resistance and slag resistance. The breathable brick can effectively protect the breathable core brick, and it is the key supporting product to ensure the smooth implementation of bottom blowing argon function. Porous plug is a kind of new product with high life, energy ...
  • High reputation JM28 Insulating Fire Brick - Al2O3-SiC-C Brick – Topower

    High reputation JM28 Insulating Fire Brick - Al2O3-SiC-C Brick – Topower

    Description AI203-SiC-C brick, referred to as ASC brick. AI203-SiC-C brick is made of fused corundum (or sintered corundum, special grade bauxite clinker), graphite and silicon carbide with fixed carbon above 90%-95% as the main raw materials. It is made by adding graphite, bauxite, and additives, after batching, forming, drying and high temperature firing. ASC brick has very good high temperature performance and anti-oxidation, anti-flaking and anti-slag erosion properties, can withsta...
  • Europe style for Magnesium Bricks - Ladle Shroud – Topower

    Europe style for Magnesium Bricks - Ladle Shroud – Topower

    Description Ladle shroud also known as the protective sleeve, is mainly used between the ladle and the tundish. It is an important part of the connection between the ladle and the tundish. The lower part of the upper connecting ladle is connected with the water outlet of the sliding nozzle device, and the lower end extends into the tundish. It prevents the molten steel entering the tundish from the ladle from being re-oxidized and splashed; protects the molten steel from secondary oxidat...
  • High Quality Alumina Silica Refractory Brick - insulation firebrick – Topower

    High Quality Alumina Silica Refractory Brick - insulation firebrick – Topower

    Description The density of insulation firebrick is 0.60~1.25g/cm3, and the working temperature is 900°C to 1600°C. Insulation firebrick can reduce the cost of the foundation, reduce the cross-section of the frame, and save reinforced concrete can significantly save the comprehensive cost of the building. Compared with solid clay bricks, the overall cost of using lightweight bricks can be reduced by more than 5%. Lightweight bricks have good work ability and are easy to construct. Feat...