Ceramic Fiber Textiles
Description
Ceramic fiber textiles have good thermal insulation performance, which is superior to traditional ceramic fiber products such as high strength, mechanical vibration resistance and impact resistance. Industrial refractory fibre is made from ceramic fibre, E-Glass Fibre,vycor fibre, PANOF, etc material, the products include yarn, cloth, tape, twisted rope, packing, tube, Coated Fabric and other kinds of tech textiles. Widely used in heat insulation sealing etc
Features
High temperature resistance, low thermal conductivity, thermal shock resistance, low heat capacity;
Excellent high temperature insulation performance and long service life;
It has the ability to resist the corrosion of non-ferrous metals such as aluminum and zinc;
Has good low temperature and high temperature strength;
Non-toxic, harmless, and has no adverse effects on the environment;
Application
Ceramic fiber textiles can be widely used in the chemical industry, electric power, paper making, food, pharmaceutical and other industries, boiler doors, high temperature, high pressure machines, pumps, valve sealing. It is suitable for clean fluid or slurry, salt water, emulsion, grease, hydrocarbon, solvent, pulp and other media.
Physical And Chemical Indicators
Brand |
Bio-Soluble fiber rope/cloth/tap/yarn |
Ceramic fiber rope/cloth/tap/yarn |
|||
GF-Rope/Cloth/ Tape/Yarn |
SS-Rope/Cloth/ Tape/Yarn |
GF-Rope/Cloth/ Tape/Yarn |
SS-Rope/Cloth/ Tape/Yarn |
||
Specification Temp. (℃) |
1260 |
||||
Working Temp. (℃) |
500-600 |
1100 |
500-600 |
1100 |
|
Bulk Density (kg/m3) |
500 |
||||
Organic matter (%) |
15 |
||||
Moisture Content(%) |
1 |
||||
Chemical Composition(%) |
SiO2 |
55-65 |
51 |
||
CaO |
23-35 |
-- |
|||
MgO |
On May 10 |
-- |
|||
Al2O3 |
-- |
45 |
|||
Fe2O3 |
-- |
0.8 |
|||
Reinforced material |
Glass Filament |
Stainless steel 304 |
Glass Filament |
Stainless steel 304 |
|
Note: Rope Dia size :(mm)6/10/12/20/25/32/38/50, Rope Shape: Round Braided Rope& Twisted Rope &Square Braided Rope |
Productive Process
1.Raw material quality control including physical and chemical testing.
2.crushing and grinding of bulk raw materials.
3.Packing after quality testing.

Packing And Shipping
Packaging according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By 25kg kraft paper bags+sea fumigated wooden pallets

1.Raw material quality control including physical and chemical testing.
2.Crushing and grinding of bulk raw materials.
3. According to customer data sheet required to mixing Raw Material.
Pressing or shaping the green brick depend on different raw material and brick shape.
4.Dry the bricks at dryer kiln.
5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
6.The quality control department will inspect the finished refractory bricks random.

Packaging according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor