Ceramic Fibre Board
Description
The strength of ceramic fiber board is higher than that of fiber blankets and vacuum forming felts, and is suitable for high-temperature fields that require rigidity and strength of products. The surface is flat, the size is accurate, the toughness is good, it can be cut at will, and the heat preservation effect is excellent. It is uniform inside and outside and has good heat insulation performance.
Features
The ceramic fiber board has the features as following:
1. Excellent thermal stability and thermal shock resistance
2. Low heat capacity
3. Low thermal conductivity
4. High compressive strength
5. Good toughness
6. Easy to process and install
Application
Ceramic fiber board is an ideal heat preservation and heat insulation material for various industrial kilns. It can be used as back lining,wall lining and lining insulation of kilns.
Refractory brick backing of electrolytic reduction tank in aluminum factory
High temperature reaction, wall lining and backing material of heating equipment
Physical And Chemical Indicators
Brand |
STBOD |
HABOD |
HZBOD |
|
Specification Temp. (℃) |
1260 |
1360 |
1430 |
|
Working Temp. (℃) |
1100 |
1200 |
1350 |
|
Bulk Density (g/cm3) |
280 |
280 |
280 |
|
Permanent linear change (%) |
-3 |
-3 |
-3 |
|
Thermal Conductivity(w/m.k) |
0.085(400℃) |
0.085(400℃) |
0.085(400℃) |
|
Cold Crushing Strength (MPa) |
0.2 |
0.2 |
0.2 |
|
Chemical Composition (%) |
Al2O3 |
43 |
51-53 |
39-40 |
Al2O3+SiO2 |
96 |
99 |
- |
|
Al2O3+SiO2+ZrO2 |
- |
- |
99 |
|
ZrO2 |
- |
- |
15-17 |
|
Fe2O3 |
1.0 |
0.5 |
0.2 |
|
Na2O+K2O |
0.5 |
0.2 |
0.2 |
1.Raw material quality control including physical and chemical testing.
Put the selected raw materials in the furnace for high temperature spinning.
2.Needle with the needling machine.
3.Cut the board into the size required by the customer.

Packaging according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor