Ceramic fiber bulk is a high-temperature refractory fiber made of high-purity raw materials through high-temperature melting, using blowing or spinning technology. The fiber has good chemical stability and can resist the erosion of most aggressive chemicals. Even if the finished product is wetted by oil, water or steam, its physical properties such as temperature resistance and heat insulation will not change. Fiber cotton can be further processed into fiber blanket, felt, board, paper, cloth, rope and other products.


Product Detail

Productive Process

PACKING AND SHIPPING

Product Tags

Description


Ceramic fiber bulk is a high-temperature refractory fiber made of high-purity raw materials through high-temperature melting, using blowing or spinning technology. The fiber has good chemical stability and can resist the erosion of most aggressive chemicals. Even if the finished product is wetted by oil, water or steam, its physical properties such as temperature resistance and heat insulation will not change. Fiber cotton can be further processed into fiber blanket, felt, board, paper, cloth, rope and other products.

Features

Light weight, anti-oxidation

Low thermal conductivity, good flexibility

White, precise size, easy to cut and install, convenient

Does not contain any adhesives, can be used for a long time in neutral and oxidizing environments

Low heat capacity, low thermal conductivity, high refractoriness and high heat sensitivity

Excellent resistance to wind erosion and mechanical shock

Excellent sound absorption and fire resistance

Stable density and performance

Application

Industrial kilns, boiler linings, lining insulation, refractory insulation

Thermal insulation of steam engines, gas engines and other thermal equipment

Flexible insulating material for high temperature pipeline; high temperature gasket; high temperature filtration

Thermal reactor insulation

Fire protection of various industrial equipment, heat insulation and fire protection of electrical components

Thermal insulation materials for incineration equipment

Materials for modules, folding blocks and veneer blocks

Thermal insulation of investment castings

Physical And Chemical Indicators

Brand / Properties

STD BULK

HP BULK

HZ BULK

Chemical Composition(%)

Al2O3

≥44

≥45

≥34

SiO2

≥52

≥54

≥50

Fe2O3

≤1.0

≤0.5

≤0.5

Na2O

≤1.0

≤0.2

≤0.2

ZrO2

-

-

≥15

Specification Temp. (℃)

1260

1260

1430

Shot content (%)

≤15

≤15

≤12

Fiber Diameter(μm)

3.5

Productive Process

1.Raw material quality control including physical and chemical testing.

2.crushing and grinding of bulk raw materials.

3.Packing after quality testing.

Packing And Shipping

Packaging according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By 25kg kraft paper bags+sea fumigated wooden pallets


  • Previous:
  • Next:

  • 1.Raw material quality control including physical and chemical testing.           
    2.Crushing and grinding of bulk raw materials.
    3. According to customer data sheet required to mixing Raw Material.
    Pressing or shaping the green brick depend on different raw material and brick shape.
    4.Dry the bricks at dryer kiln.
    5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
    6.The quality control department will inspect the finished refractory bricks random.

    Packaging  according to safety sea-exporting packing Standard
    Dispatch : loading the finished packing material at factory by container Door toDoor   
    By sea fumigated wooden pallet + plastic belt  + plastic film wrap.

    Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.