Ceramic Fibre Module

Short Description:

The ceramic fiber module is a new type of refractory lining product introduced to simplify and speed up the construction of the kiln and improve the integrity of the lining. The product is white in color and regular in size. It can be directly fixed on the anchor nails of the steel plate of the industrial kiln shell. It has a good fire-resistant and heat-insulating effect, which improves the integrity of the fire-resistant and heat-insulating kiln and promotes the progress of kiln masonry technology .


Product Detail

Productive Process

PACKING AND SHIPPING

Product Tags

Description


The ceramic fiber module is a new type of refractory lining product introduced to simplify and speed up the construction of the kiln and improve the integrity of the lining. The product is white in color and regular in size. It can be directly fixed on the anchor nails of the steel plate of the industrial kiln shell. It has a good fire-resistant and heat-insulating effect, which improves the integrity of the fire-resistant and heat-insulating kiln and promotes the progress of kiln masonry technology .

The ceramic fiber module has excellent chemical stability; excellent thermal stability; excellent elasticity. The ceramic fiber module is in a preloaded state. After the furnace lining is built, the expansion of the ceramic fiber module makes the furnace lining seamless and can compensate for the fiber furnace lining Shrink to improve the thermal insulation performance of the fiber lining, and the overall performance is good; excellent thermal stability and thermal shock resistance; the ceramic fiber module is installed quickly, and the anchors are set on the cold surface of the wall lining, which can reduce the requirements for anchor materials.

Features

Low bulk density, low thermal conductivity

Resistance to thermal shock and airflow

High mechanical strength, built-in anchors, good safety performance

The installation is simple, the furnace lining forms a seamless whole after installation, and the thermal insulation effect is good

Application

Ceramic industry: tunnel kiln, shuttle kiln, roller kiln

Petrochemical industry: atmospheric furnace, conversion furnace, coking furnace, cracking furnace, heating furnace, flue, etc.

Iron and steel industry: ladle cover, heating furnace, annealing furnace, bell furnace, walking furnace, hot blast pipe and pipe, etc.

Environmental protection and energy saving industry: waste incinerator, RTO exhaust gas treatment furnace, SCR environmental protection catalytic furnace, etc.

Physical And Chemical Indicators

Brand / Properties

STD Module

HP Module

HZ Module

ChemicalComposition(%)

Al2O3

≥44

≥45

≥34

SiO2

≥52

≥54

≥50

Fe2O3+TiO2

≤1.0

≤0.5

≤0.5

ZrO2

-

-

≥15

K2O+Na2O+Fe2O3

≤1.0

≤0.2

≤0.2

Bulk Density (kg/m3)

220

220

220

Specification Temp. (℃)

1260

1350

1430

Linear Shrinkage after Heatin%

1000℃X24h≤2.5

1000℃X24h≤2.5

1000℃X24h≤3.5

Thermal Conductivity(w/m.k)

400℃

0.09

0.101

0.118

500℃

0.119

0.12

0.149

600℃

0.152

0.175

0.172

Productive Process

1.Raw material quality control including physical and chemical testing.

2.crushing and grinding of bulk raw materials.

3.Packing after quality testing.

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By 25kg kraft paper bags+sea fumigated wooden pallets


  • Previous:
  • Next:

  • 1.Raw material quality control including physical and chemical testing.           
    2.Crushing and grinding of bulk raw materials.
    3. According to customer data sheet required to mixing Raw Material.
    Pressing or shaping the green brick depend on different raw material and brick shape.
    4.Dry the bricks at dryer kiln.
    5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
    6.The quality control department will inspect the finished refractory bricks random.

    Packaging  according to safety sea-exporting packing Standard
    Dispatch : loading the finished packing material at factory by container Door toDoor   
    By sea fumigated wooden pallet + plastic belt  + plastic film wrap.

  • Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.