Chamotte

Short Description:

Chamotte is a high-quality hard refractory clay produced in Zibo, Shandong Province, China. The standard Al2O3 content of chamotte ore is 38%, after calcination the Al2O3 content is about 44%, and Fe2O3<2%. The composition is stable, the texture is uniform, the structure is dense, and the section is shell-shaped and white. It is used to produce high-quality clay refractory materials. The technical term is the first-grade hard clay clinker, the main chemical components are AL2O3 and SiO2, accompanied by a small amount of Fe2O3 and trace amounts of Na2O and K2O. The main mineral is kaolin.

The chamotte we call generally refer to CALCINED CLAY. . The content of Al2O3 in the calcined chamotte is about 44%, and the content of Fe2O3 is not more than 2%. The composition is stable, the texture is uniform, the structure is dense, and the section is shell-shaped.

The common colors of chamotte after high temperature calcination are: pure white, light gray, light yellow brown, and a small amount of brown iron sheet.


Product Detail

Product Tags

Description


Chamotte is a high-quality hard refractory clay produced in Zibo, Shandong Province, China. The standard Al2O3 content of chamotte ore is 38%, after calcination the Al2O3 content is about 44%, and Fe2O3<2%. The composition is stable, the texture is uniform, the structure is dense, and the section is shell-shaped and white. It is used to produce high-quality clay refractory materials. The technical term is the first-grade hard clay clinker, the main chemical components are AL2O3 and SiO2, accompanied by a small amount of Fe2O3 and trace amounts of Na2O and K2O. The main mineral is kaolin.

The chamotte we call generally refer to CALCINED CLAY. . The content of Al2O3 in the calcined chamotte is about 44%, and the content of Fe2O3 is not more than 2%. The composition is stable, the texture is uniform, the structure is dense, and the section is shell-shaped.

The common colors of chamotte after high temperature calcination are: pure white, light gray, light yellow brown, and a small amount of brown iron sheet.

Features

Chamotte are not easily dispersed in water and have low plasticity.

Chamotte have heat resistance and sinterability

After being calcined at high temperature, the scorched gem has the characteristics of stable volume, high strength and low water absorption.

Application

Chamotte are used in the production of advanced refractory materials, ceramics, aluminum silicate refractory fiber production and military industry.

It is widely used in metallurgy, casting, chemical, ceramics, electric power, machinery, petroleum and other industries.

Physical And Chemical Indicators

         Brand
   Properties           

YNS45

YNS45

YNS44

YNS44

YNS43

YNS42

YNS40

A

B

A

B

AL2O3 %

46

45

44

44

43

42

40

SiO2 %

49-52

49-52

50-53

50-53

50

50

50

Fe2O3 %    

1

1.15

1.3

1.5

2

2.5

3

TiO2 %    

0.8

0.8

0.9

0.9

1

1.1

1.2

 K2O+Na2O %    

0.3

0.3

0.4

0.4

0.4

0.5

0.5

CaO+MgO %    

0.5

0.5

0.5

0.5

0.5

0.6

0.7

Bulk density g/cm³ 

2.58

2.55

2.52

2.5

2.45

2.4

2.37

Refractoriness °C 

1780

1770

1760

1750

1740

1720

1710

Productive Process

1.Raw material quality control including physical and chemical testing.

2.crushing and grinding of bulk raw materials.

3.Packing after quality testing

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By 25kg kraft paper bags+sea fumigated wooden pallets