Our primary objective is always to offer our clients a serious and responsible small business relationship, offering personalized attention to all of them for Stainless Steel Masonry Anchors, Magnesia Carbon Brick, Firebrick Mortar Mix, Now we have established steady and long business relationships with customers from North America, Western Europe, Africa, South America, more than 60 countries and regions.
Excellent quality Stainless Steel Sleeve Anchors - Soluble Fiber Board – Topower Detail:

Description

Soluble fiber board is made of soluble fiber cotton, refractory fillers, a small amount of organic binders and inorganic binders, and has excellent thermal insulation and processing properties.
Soluble fiber board is made of soluble fiber cotton, refractory fillers, a small amount of organic binders and inorganic binders, and has excellent thermal insulation and processing properties.

Features

Environmental protection and high safety, soluble and biodegradable / Softer texture and less irritation / Lower shot content

Can resist far infrared radiation, lower thermal conductivity / Better thermal stability / Stronger chemical resistance

Good heat resistance / Low thermal conductivity, low heat capacity / Flat appearance, accurate size, easy to install and use

Application

Insulation of household thermal equipment, such as thermal storage electric heaters, ovens

Civil building exterior wall insulation and elevator door fire protection

Insulation layer of various environmental protection equipment and mine life-saving equipment

Refractory layer or insulation lining of various industrial furnace equipment

Furnace door sealing, flange sealing, pipe insulation

Thermal insulation of industrial energy storage equipment

Heat insulation, sound insulation and noise reduction of automobile exhaust system

Fire and heat insulation of marine drilling platforms and ships

High temperature and heat insulation in nuclear power field

Physical And Chemical Indicators

Brand / Properties

 Soluble fiber board

Specification Temp. (℃)

1260

Working Temp. (℃)

1100

Bulk Density (kg/m3)

280

Linear Shrinkage after Heating @24hours

-4
(1000℃)

Thermal Conductivity (w/m.k)

0.153(500℃)

Tensile Strength (MPa)

0.1

Moisture content  (%)

1

Organic matter  (%)

6

Productive Process

1.Raw material quality control including physical and chemical testing.

Put the selected raw materials in the furnace for high temperature spinning.

2.Needle with the needling machine.

3.Cut the board into the size required by the customer.

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By hard paper carton(Outside)+plastic bags(inside).


Product detail pictures:

Excellent quality Stainless Steel Sleeve Anchors - Soluble Fiber Board – Topower detail pictures

Excellent quality Stainless Steel Sleeve Anchors - Soluble Fiber Board – Topower detail pictures

Excellent quality Stainless Steel Sleeve Anchors - Soluble Fiber Board – Topower detail pictures


Related Product Guide:

We take "customer-friendly, quality-oriented, integrative, innovative" as objectives. "Truth and honesty" is our administration ideal for Excellent quality Stainless Steel Sleeve Anchors - Soluble Fiber Board – Topower , The product will supply to all over the world, such as: UK, Nepal, San Francisco, Our products are widely sold to Europe, USA, Russia, UK, France, Australia, Middle East, South America, Africa, and Southeast Asia, etc. Our products are highly recognized by our customers from all around the world. And our company is committed to continually improving effectiveness of our management system to maximize customer satisfaction. We sincerely hope to make progress with our customers and create a win-win future together. Welcome to join us for business!
  • We are long-term partners, there is no disappointment every time, we hope to maintain this friendship later!
    5 Stars By Fay from Ecuador - 2017.09.22 11:32
    As a veteran of this industry, we can say that the company can be a leader in the industry, select them is right.
    5 Stars By Heather from Manchester - 2017.12.19 11:10
    Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.