Factory For Castable Refractory Cement - Insulating Castable Refractories – Topower

Factory For Castable Refractory Cement - Insulating Castable Refractories – Topower

Short Description:


Product Detail

Product Tags

Related Video

Feedback (2)

So that you can finest fulfill client's demands, all of our operations are strictly performed in line with our motto "High Excellent, Competitive Price, Fast Service" for Calcium Silicate Board Australia, Castable Refractory Cement Forge, Magnesia Refractory Bricks, We give priority to quality and customer satisfaction and for this we follow stringent quality control measures. We have in-house testing facilities where our products are tested on every aspect at different processing stages. Owning to latest technologies, we facilitate our customers with customized production facility.
Factory For Castable Refractory Cement - Insulating Castable Refractories – Topower Detail:

Description

Insulation refractory castable have light bulk density, low thermal conductivity, high strength, uniform air tightness, and are resistant to acids and alkalis. It is suitable for the furnace body, furnace wall and furnace roof of medium and low temperature thermal equipment. After being cast on site, the insulation layer becomes a whole and the insulation performance is enhanced. It is used on various power station boilers and industrial kilns. Excellent heat insulation and energy saving effect.

Features

Low bulk density / Low thermal conductivity / Good insulation performance

Strong overall performance / Good thermal shock resistance / long lasting / Simple construction

Application

Insulation refractory castable is widely used in the insulation parts of industrial kilns and thermal equipment in metallurgy, machinery, electric power, petroleum, chemical and other industries.

Insulation refractory castable is suitable for the refractory and heat-insulating lining of petrochemical tube furnaces, as well as the refractory and heat-insulating lining of various heating furnace bottoms, furnace walls, flue chimneys, radiation chambers, convection chambers, elbow boxes, and cracking of ethylene crackers Furnace lining. At the same time, it can also be applied to the insulation layer of other high-temperature furnaces.

Physical And Chemical Indicators

Brand
   Properties

LWC-170

LWC-160

LWC-150

LWC-140

LWC-130

LWC-120

Application Limit Temp ℃

1,700

1,600

1,500

1,400

1,200

1,100

Bulk Density (g/cm3)

1.45

1.5

1.55

1.45

1.25

1.15

Water Required for Casting (%)

18-23

20-25

21-25

28-35

40-45

45-50

CCS/MOR(MPa)

at110℃x24h

15(4)

10(3.0)

12(3.5)

11(3.3)

8(3)

8(2.5)

at1,200℃x3h

14(4)

10(3.0)

11(3.5)

5(2.5)

4(2)

4(2)
at1,000℃

at1,400℃x3h

15(5)

14(8.1)

22(10.8)

15(3)

-

-

Permanent Linear Change (%)

at110℃x24h

-0.08

-0.06

-0.12

-0.06

-0.09

-0.09

at1,200℃x3h

-0.1

-0.1

-0.18

-0.4

-0.8

-0.65
at1,000℃

at1,400℃x3h

0.1

-0.5

0.1

-1.0

-

-

Thermal conductivity(W/m.k)

at400℃

0.6

0.5

0.52

0.32

0.18

0.16

at1,000℃

0.8

0.6

0.64

0.41

0.24

0.21

Chemical Analysis(%) 

Al2O3

90

75

60

43

35

33

SiO2

-

15

30

40

47

49

Productive Process

1.Raw material quality control including physical and chemical testing.

2.crushing and grinding of bulk raw materials.

3.Packing after quality testing.

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard

Dispatch : loading the finished packing material at factory by container Door toDoor

By 25kg kraft paper bags+sea fumigated wooden pallets


Product detail pictures:

Factory For Castable Refractory Cement - Insulating Castable Refractories – Topower detail pictures

Factory For Castable Refractory Cement - Insulating Castable Refractories – Topower detail pictures

Factory For Castable Refractory Cement - Insulating Castable Refractories – Topower detail pictures


Related Product Guide:

It adheres on the tenet "Honest, industrious, enterprising, innovative" to acquire new solutions regularly. It regards shoppers, success as its very own success. Let us establish prosperous future hand in hand for Factory For Castable Refractory Cement - Insulating Castable Refractories – Topower , The product will supply to all over the world, such as: Singapore, Qatar, Atlanta, Whether selecting a current product from our catalog or seeking engineering assistance for your application, you can talk to our customer service center about your sourcing requirements. We are looking forward to cooperating with friends from all over the world.
  • With a positive attitude of "regard the market, regard the custom, regard the science", the company works actively to do research and development. Hope we have a future business relationships and achieving mutual success.
    5 Stars By Giselle from Congo - 2018.09.16 11:31
    Products and services are very good, our leader is very satisfied with this procurement, it is better than we expected,
    5 Stars By Dolores from Hongkong - 2018.11.02 11:11
    Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.