Mullite Insulation Bricks

Q1: What density could produce for light weight mullite insulation bricks?

A1: The minimum density could do is 0.5g/cm3,the max is 1.3g/cm3.Standard is 0.6,0.8,0.9,1.0,1.1g/cm3 etc…

 

Q2: What is the firing temperature for mullite insulating brick?

A2: Firing temperature or JM23 is 1300C,and 1400C for Jm26,1500C for JM28.

 

Q3: What is the main application area for mullite insulating bricks?

A3: Its application is widely,mainly in ceramic kiln,steel plant and insulation lining in kiln,it also can contact fire directly.

Ceramic Fiber Blanket & Board

Q1: Do you export any of your products to Europe? What are the products?

A1: Yes, our products are exported to Europe. Like RHI, Calderys and Intocast are all our customers. We export firebrick, magnesia chrome brick and insulation material to them.

 

Q2: Could you tell me the loading quantity of your ceramic fiber blanket for full container?

A2: Yes, please refer to the FCL quantity below.

CF blanket

              Packaging Qty(rolls)

Temp

B/D

Size

(mm)

U.W.

(Kg/pc)

Rolls /Pallet

20 GP

40 HQ

1260

96

14400x610x13

10.96

16/20/pallet

160

420

1260

96

7200x610x19

8.01

16/20/pallet

160

420

1260

96

7200x610x25

10.54

16/20/pallet

160

420

1260

96

3600x610x50

10.54

16/20/pallet

160

420

1260

128

14400x610x13

14.62

16/20/pallet

160

420

1260

128

7200x610x19

10.68

16/20/pallet

160

420

1260

128

7200x610x25

14.05

16/20/pallet

160

420

1260

128

3600x610x50

14.05

16/20/pallet

160

420

1400

128

14400x610x13

14.62

16/20/pallet

160

420

1400

128

7200x610x19

10.68

16/20/pallet

160

420

1400

128

7200x610x25

14.05

16/20/pallet

160

420

1400

128

3600x610x50

14.05

16/20/pallet

160

420

Q3: Could you provide the loading quantity of your Ceramic Fiber Board for full container?

A3: Yes, please refer to the FCL quantity below.

CF board

              Packaging Qty(pcs)

Temp

B/D

Size

(mm)

U.W.

(Kg/pc)

Pieces /Pallet

20 GP

40 HQ

1260

300

1000x500x15

2.25

300/354/pallet

3000

8496

1260

300

1000x500x30

4.5

150/176/pallet

1500

4224

1260

300

1000x500x40

6

112/132/pallet

1120

3168

1260

300

1000x500x50

7.5

90/104/pallet

900

2496

1260

300

1000x500x60

9

74/88/pallet

740

2112

1260

300

1000x500x70

10.5

64/74/pallet

640

1776

Ceramic Fiber Rope

Q1: How many types rope do you have?

A1: For shape normal we have two types: round rope and square rope.

For material normal we have two types: rope with stainless steel wire reinforcement and rope with fiberglass reinforcement.

 

Q2: How was the difference of the rope with stainless steel wire reinforcement and rope with fiberglass reinforcement?

A2:

1.Stainless steel wire reinforcement,working temp is about 1050℃-1100℃,because the highest working temp of Stainless steel is around 1050℃.

2.Fiberglass reinforcement,working temp can arrive 550℃-650℃,because the highest working temp of Fiberglass is around 600℃.

 

 

Q3: How was the packing with the rope?

A3: Normally the packing is plastic protective film+woven bag. If requested we can customize hard card carton for customers with required Logo, charges separate calculate according actual situation.

Bricks for rotary kiln

Q1: For the rotary kiln(such as cement kiln or lime kiln etc.),can do design the whole kiln?

A1: Yes,of course.We have the professional engineer teams,we not only can provide our designing scheme showing each zone used specification and sizes,but also we can provide the installation manual.

( Bricks for cement kiln mainly include: Magnesia chorme brick,Magnesia spinel brick & hercynite brick )

Inspect Factories

Q1: Because of the epidemic, we can’t go to China to inspect factories. Do you have any solutions?

A1: We can make an appointment, and then we can inspect the plant by video.

Let you know our factory and production details. This can also save some travel expenses.

Quality Of Products

Q1: How do u you guarantee the quality of your products?

A1: We have full quality assurance system and experienced quality inspectors, before producing we will test the raw material and after finished we will do the physical and chemical testing for every , and will send the report to you.

You can also ask the third party inspection to do the test if u have any doubt.

WANT TO WORK WITH US?