High definition Stainless Steel Bruce Anchor - Ceramic Fibre Module – Topower

High definition Stainless Steel Bruce Anchor - Ceramic Fibre Module – Topower

Short Description:


Product Detail

Product Tags

Related Video

Feedback (2)

Our workforce through professional training. Skilled professional knowledge, solid sense of service, to fulfill the services demands of consumers for Firebrick Insulation, Concrete Retaining Wall Slabs, Precast Concrete Louvers, In case you are intrigued in almost any of our merchandise, remember to will not hesitate to make contact with us and take the initial step to create up a prosperous enterprise romance.
High definition Stainless Steel Bruce Anchor - Ceramic Fibre Module – Topower Detail:

Description

The ceramic fiber module is a new type of refractory lining product introduced to simplify and speed up the construction of the kiln and improve the integrity of the lining. The product is white in color and regular in size. It can be directly fixed on the anchor nails of the steel plate of the industrial kiln shell. It has a good fire-resistant and heat-insulating effect, which improves the integrity of the fire-resistant and heat-insulating kiln and promotes the progress of kiln masonry technology .

The ceramic fiber module has excellent chemical stability; excellent thermal stability; excellent elasticity. The ceramic fiber module is in a preloaded state. After the furnace lining is built, the expansion of the ceramic fiber module makes the furnace lining seamless and can compensate for the fiber furnace lining Shrink to improve the thermal insulation performance of the fiber lining, and the overall performance is good; excellent thermal stability and thermal shock resistance; the ceramic fiber module is installed quickly, and the anchors are set on the cold surface of the wall lining, which can reduce the requirements for anchor materials.

Features

Low bulk density, low thermal conductivity

Resistance to thermal shock and airflow

High mechanical strength, built-in anchors, good safety performance

The installation is simple, the furnace lining forms a seamless whole after installation, and the thermal insulation effect is good

Application

Ceramic industry: tunnel kiln, shuttle kiln, roller kiln

Petrochemical industry: atmospheric furnace, conversion furnace, coking furnace, cracking furnace, heating furnace, flue, etc.

Iron and steel industry: ladle cover, heating furnace, annealing furnace, bell furnace, walking furnace, hot blast pipe and pipe, etc.

Environmental protection and energy saving industry: waste incinerator, RTO exhaust gas treatment furnace, SCR environmental protection catalytic furnace, etc.

Physical And Chemical Indicators

Brand / Properties

STD Module

HP Module

HZ Module

ChemicalComposition(%)

Al2O3

≥44

≥45

≥34

SiO2

≥52

≥54

≥50

Fe2O3+TiO2

≤1.0

≤0.5

≤0.5

ZrO2

-

-

≥15

K2O+Na2O+Fe2O3

≤1.0

≤0.2

≤0.2

Bulk Density (kg/m3)

220

220

220

Specification Temp. (℃)

1260

1350

1430

Linear Shrinkage after Heatin(%)

1000℃X24h≤2.5

1000℃X24h≤2.5

1000℃X24h≤3.5

Thermal Conductivity(w/m.k)

400℃

0.09

0.101

0.118

500℃

0.119

0.12

0.149

600℃

0.152

0.175

0.172

Productive Process

1.Raw material quality control including physical and chemical testing.

2.crushing and grinding of bulk raw materials.

3.Packing after quality testing.

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By 25kg kraft paper bags+sea fumigated wooden pallets


Product detail pictures:

High definition Stainless Steel Bruce Anchor - Ceramic Fibre Module – Topower detail pictures

High definition Stainless Steel Bruce Anchor - Ceramic Fibre Module – Topower detail pictures

High definition Stainless Steel Bruce Anchor - Ceramic Fibre Module – Topower detail pictures


Related Product Guide:

With this motto in mind, we've come to be one of quite possibly the most technologically innovative, cost-efficient, and price-competitive manufacturers for High definition Stainless Steel Bruce Anchor - Ceramic Fibre Module – Topower , The product will supply to all over the world, such as: Turkmenistan, Saudi Arabia, Argentina, During in 11 years,We have participated in more than 20 exhibitions,obtains the highest praise from each customer. Our company always aim to provide the customer best products with lowest price. We are making great efforts to achieve this win-win situation and sincerely welcome you to join us. Join us, show your beauty. We will always be your first choice. Trust us, you will never lose heart.
  • The factory technical staff gave us a lot of good advice in the cooperation process, this is very good, we are very grateful.
    5 Stars By Prudence from US - 2018.12.25 12:43
    The supplier abide the theory of "quality the basic, trust the first and management the advanced" so that they can ensure a reliable product quality and stable customers.
    5 Stars By Doris from Jakarta - 2018.11.11 19:52
    Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.