Our primary intention should be to offer our clientele a serious and responsible enterprise relationship, delivering personalized attention to all of them for Chamotte Stone, Magnesia Brick, Refractory Mortar, We warmly welcome all standpoint inquiries from home and abroad to cooperate with us, and anticipate your correspondence.
High definition Stainless Steel Bruce Anchor - Ceramic Fibre Paper – Topower Detail:

Description

The ceramic fiber blanket is made by high-temperature melt spraying or spinning of raw materials into fibers, and is made by double-sided needle punching. The color is white, the size is regular, and it integrates fire resistance, heat insulation and heat preservation functions. The ceramic fiber blanket can maintain good tensile strength, toughness and fiber structure when used in a neutral and oxidizing atmosphere.

After the double-sided needling process, the degree of fiber interweaving, delamination resistance, tensile strength and surface flatness are greatly improved. The fiber blanket does not contain any organic bonding agent to ensure that the ceramic fiber blanket has good manufacturability and stability under high temperature and low temperature conditions.

The ceramic fiber blanket is white in color and regular in size. It integrates fire resistance, heat insulation and heat preservation, and does not contain a binder. When used in a neutral, oxidizing atmosphere, it can maintain good tensile strength, toughness and fiber structure. Temperature resistance is 950-1400℃, with chemical stability, thermal stability, sound absorption and noise reduction performance, high tensile strength, low thermal conductivity, low heat capacity, etc.

Features

1.Low thermal conductivity

2. low heat capacity

3. thermal shock resistance

4. good flexibility, tear resistance

5. does not contain asbestos, does not act with liquid aluminum

6. good electrical insulation and sound insulation performance

7. good mechanical processing performance

8. tough texture, high compressive strength

Application

Ceramic fiber paper is widely used in all kinds of industrial furnace and ladle, the ladle, submerged nozzle of high temperature heat insulation material, industrial furnace electric insulation and heat insulation material, the oven door and furnace expansion joint sealing material, aluminum model lining, microcrystalline glass with hot melt glass membrane, high temperature sealing gasket, instruments and equipment heating device of insulation and electrical insulating materials, acoustical insulation of automobile muffler, the exhaust pipe thermal insulation materials, isolation of sintering materials, warming my hands treasure insulation, straightening roll, hair heat insulation, electrical and electronic insulating.

Physical And Chemical Indicators

Brand Properties

DK-1260

DK-1350

DK-1430

Specification Temp (℃)

1000

1100

1300

Bulk Density (kg/m3)

200

200

200

Tensile strength (MPa)

0.4

Organic matter content(%)

≤8

Thickness (mm)

0.5-10mm

Width (mm)

610mm  1220mm

ChemicalComposition(%)

Al2O3

47

48

40

SiO2

52

51

15-17 ZrO2

Fe2O3

0.5

0.5

0.2

NaO2

0.2

 0.2

0.2

Productive Process

1.Raw material quality control including physical and chemical testing.

Put the selected raw materials in the furnace for high temperature spinning.

2.Needle with the needling machine.

3.Roll up the woven blanket.

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By hard paper carton(Outside)+plastic bags(inside).


Product detail pictures:

High definition Stainless Steel Bruce Anchor - Ceramic Fibre Paper – Topower detail pictures

High definition Stainless Steel Bruce Anchor - Ceramic Fibre Paper – Topower detail pictures

High definition Stainless Steel Bruce Anchor - Ceramic Fibre Paper – Topower detail pictures


Related Product Guide:

In the past few years, our company absorbed and digested advanced technologies both at home and abroad. Meanwhile, our company staffs a team of experts devoted to the development of High definition Stainless Steel Bruce Anchor - Ceramic Fibre Paper – Topower , The product will supply to all over the world, such as: Ghana, Tunisia, Estonia, With the superior and exceptional service, we've been well developed along with our customers. Expertise and know-how ensure that we are always enjoying the trust from our customers in our business activities. "Quality", "honesty" and "service" is our principle. Our loyalty and commitments remain respectfully at your service. Contact Us Today For further information, contact us now.
  • We have been appreciated the Chinese manufacturing, this time also did not let us disappoint,good job!
    5 Stars By Kama from Bolivia - 2018.10.01 14:14
    This supplier's raw material quality is stable and reliable, has always been in accordance with the requirements of our company to provide the goods that quality meet our requirements.
    5 Stars By Nancy from Philippines - 2017.06.22 12:49
    Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.