It adheres on the tenet "Honest, industrious, enterprising, innovative" to acquire new solutions regularly. It regards shoppers, success as its very own success. Let us establish prosperous future hand in hand for Mullite Composition, Bauxite Mining, Andalusite, We aim at Ongoing system innovation, management innovation, elite innovation and market innovation, give full play to the overall advantages, and constantly improve service quality.
Hot-selling Stainless Steel Concrete Anchors - Ceramic Fibre Bulk – Topower Detail:

Description

Ceramic fiber bulk is a high-temperature refractory fiber made of high-purity raw materials through high-temperature melting, using blowing or spinning technology. The fiber has good chemical stability and can resist the erosion of most aggressive chemicals. Even if the finished product is wetted by oil, water or steam, its physical properties such as temperature resistance and heat insulation will not change. Fiber cotton can be further processed into fiber blanket, felt, board, paper, cloth, rope and other products.

Features

Light weight, anti-oxidation

Low thermal conductivity, good flexibility

White, precise size, easy to cut and install, convenient

Does not contain any adhesives, can be used for a long time in neutral and oxidizing environments

Low heat capacity, low thermal conductivity, high refractoriness and high heat sensitivity

Excellent resistance to wind erosion and mechanical shock

Excellent sound absorption and fire resistance

Stable density and performance

Application

Industrial kilns, boiler linings, lining insulation, refractory insulation

Thermal insulation of steam engines, gas engines and other thermal equipment

Flexible insulating material for high temperature pipeline; high temperature gasket; high temperature filtration

Thermal reactor insulation

Fire protection of various industrial equipment, heat insulation and fire protection of electrical components

Thermal insulation materials for incineration equipment

Materials for modules, folding blocks and veneer blocks

Thermal insulation of investment castings

Physical And Chemical Indicators

Brand / Properties

STD BULK

HP BULK

HZ BULK

Chemical Composition(%)

Al2O3

≥44

≥45

≥34

SiO2

≥52

≥54

≥50

Fe2O3

≤1.0

≤0.5

≤0.5

Na2O

≤1.0

≤0.2

≤0.2

ZrO2

-

-

≥15

Specification Temp. (℃)

1260

1260

1430

Shot content (%)

≤15

≤15

≤12

Fiber Diameter(μm)

3.5

Productive Process

1.Raw material quality control including physical and chemical testing.

2.crushing and grinding of bulk raw materials.

3.Packing after quality testing.

Packing And Shipping

Packaging according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By 25kg kraft paper bags+sea fumigated wooden pallets


Product detail pictures:

Hot-selling Stainless Steel Concrete Anchors - Ceramic Fibre Bulk – Topower detail pictures

Hot-selling Stainless Steel Concrete Anchors - Ceramic Fibre Bulk – Topower detail pictures

Hot-selling Stainless Steel Concrete Anchors - Ceramic Fibre Bulk – Topower detail pictures


Related Product Guide:

"Sincerity, Innovation, Rigorousness, and Efficiency" is definitely the persistent conception of our corporation to the long-term to establish alongside one another with customers for mutual reciprocity and mutual profit for Hot-selling Stainless Steel Concrete Anchors - Ceramic Fibre Bulk – Topower , The product will supply to all over the world, such as: Barbados, Singapore, Malawi, As a way to make use of the resource on the expanding information and facts in international trade, we welcome prospects from everywhere on the web and offline. In spite in the top quality products and solutions we supply, effective and satisfying consultation service is supplied by our professional after-sale service group. Solution lists and thorough parameters and any other info weil be sent for you timely for the inquiries. So make sure you get in touch with us by sending us emails or contact us if you have any concerns about our firm. ou can also get our address info from our web site and come to our enterprise. or a field survey of our solutions. We're confident that we have been going to share mutual results and build solid co-operation relations with our companions in this market. We're looking forward to your inquiries.
  • The factory workers have rich industry knowledge and operational experience, we learned a lot in working with them,we are extremely grateful that we can encount a good company has excellent wokers.
    5 Stars By Katherine from Yemen - 2018.06.30 17:29
    This manufacturer can keep improving and perfecting products and service, it is in line with the rules of market competition, a competitive company.
    5 Stars By Amy from Ethiopia - 2017.09.09 10:18
    Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.