insulation firebrick

Short Description:

The density of insulation firebrick is 0.60~1.25g/cm3, and the working temperature is 900°C to 1600°C. Insulation firebrick can reduce the cost of the foundation, reduce the cross-section of the frame, and save reinforced concrete can significantly save the comprehensive cost of the building. Compared with solid clay bricks, the overall cost of using lightweight bricks can be reduced by more than 5%. Lightweight bricks have good work ability and are easy to construct.


Product Detail

PRODUCTIVE PROCESS

PACKING AND SHIPPING

Product Tags

Description


The density of insulation firebrick is 0.60~1.25g/cm3, and the working temperature is 900°C to 1600°C. Insulation firebrick can reduce the cost of the foundation, reduce the cross-section of the frame, and save reinforced concrete can significantly save the comprehensive cost of the building. Compared with solid clay bricks, the overall cost of using lightweight bricks can be reduced by more than 5%. Lightweight bricks have good work ability and are easy to construct.

Features

Lower thermal conductivity / Lower bulk density

Light weight / Lower creep rate in high temp

Good thermal shock resistance performance

Application

Insulation firebrick can be used for the back insulation of hot surface refractory lining or other refractory materials; it can also be used as refractory lining or insulation material for petroleum and chemical kilns

Physical And Chemical Indicators

Description

DN-17

DN14

DN12

SK34

SK33

SK32

Refractoriness (SK)

34

34

34

34

33

32

Bulk density (g/cm3)

2.25

2.34

2.40

2.20

2.17

2.15

Cold Crushing Strength (MPa)

50

65

70

40

35

30

Apparent Porosity(%)

17

14

12

23

24

26

Permanent linear change @1400ºC*2hrs(%)

±0.1~-0.2

±0.1~-0.2

±0.1~-0.2

±0.3

±0.5

±0.5

Thermal Linear expansion @1000ºC

0.6

0.6

0.5

0.6

0.6

0.6

Refractoriness under Load (ºC)@0.2MPa

1430

1470

1500

1350

1300

1250

Chemical Analysis (%) Al2O3

42

45

46

42

38

35

Fe2O3

1.7

1.5

1.3

2.0

2.2

3.0


  • Previous:
  • Next:

  • 1.Raw material quality control including physical and chemical testing.           
    2.Crushing and grinding of bulk raw materials.
    3. According to customer data sheet required to mixing Raw Material.
    Pressing or shaping the green brick depend on different raw material and brick shape.
    4.Dry the bricks at dryer kiln.
    5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
    6.The quality control department will inspect the finished refractory bricks random.

    Packaging  according to safety sea-exporting packing Standard
    Dispatch : loading the finished packing material at factory by container Door toDoor   
    By sea fumigated wooden pallet + plastic belt  + plastic film wrap.