Ladle Shroud

Short Description:

Ladle shroud also known as the protective sleeve, is mainly used between the ladle and the tundish. It is an important part of the connection between the ladle and the tundish. The lower part of the upper connecting ladle is connected with the water outlet of the sliding nozzle device, and the lower end extends into the tundish. It prevents the molten steel entering the tundish from the ladle from being re-oxidized and splashed; protects the molten steel from secondary oxidation during casting, improves the quality of the molten steel; reduces the deposition of oxide products in the steel on the inner wall of the nozzle, and extends the service life.


Product Detail

Product Tags

Description

Ladle shroud also known as the protective sleeve, is mainly used between the ladle and the tundish. It is an important part of the connection between the ladle and the tundish. The lower part of the upper connecting ladle is connected with the water outlet of the sliding nozzle device, and the lower end extends into the tundish. It prevents the molten steel entering the tundish from the ladle from being re-oxidized and splashed; protects the molten steel from secondary oxidation during casting, improves the quality of the molten steel; reduces the deposition of oxide products in the steel on the inner wall of the nozzle, and extends the service life.

Ladle shroud is an important refractory material for maintaining casting and improving the quality of steel. The length of it is generally 600-1800mm, and the pipe diameter is 90-150 mm. Its use conditions are harsh and must have the following functions: excellent thermal shock resistance; good mechanical strength; excellent resistance to alternating corrosion of molten steel and molten slag, and high oxidation resistance.

Features

Has good thermal shock resistance

Has good corrosion resistance to molten steel and slag

Has good mechanical strength and vibration resistance

Argon sealing device must be provided at the connection of the long nozzle

Application

steel ladle,refining ladle,electric furnace refining ladle,tundish

Physical And Chemical Indicators

Brand / Properties

Ladle Shroud

Body

Slag Line

Head

Chemical Composition (%) 

Al2O3

61.02

--

38

Fe2O3

1.3

--

--

SiO2

12.8

    --

22.47

TiO2

1.59

--

--

ZrO2

--

75.1

1.2

CaO

--

1.71

--

MgO

--

--

--

LOI (%)

23.28

15.01

34.52

Bulk Density (g/cm3)

2.57

3.78

2.2

Apparent Porosity (%)

15.67

15.61

14.67

Fracture Strength (MPa)

6.9

6.97

5.32

Main Application

Ladle & Tundish