Low Cement Castable

Low Cement Castable

Short Description:

Low cement castable refers to a castable with a lower amount of cement. The cement dosage of refractory cement castables is generally 15% to 20%, and the cement dosage of low cement castables is about 5%, and some even reduce to 1% to 2%. The purpose of reducing the amount of cement is to improve the fire resistance of the castable.


Product Detail

Productive Process

Packing And Shipping

Product Tags

Description

Low cement castable refers to a castable with a lower amount of cement. The cement dosage of refractory cement castables is generally 15% to 20%, and the cement dosage of low cement castables is about 5%, and some even reduce to 1% to 2%. The purpose of reducing the amount of cement is to improve the fire resistance of the castable.

Low-cement castable is a high-tech refractory developed on common castables by using rheological principles, the tightest packing theory and ultra-fine powder technology. It has the characteristics of low porosity, small pore size, high density, good volume stability, high strength and small water addition, and overcomes the characteristics of a significant decrease in strength of ordinary castables at 800~1200, and increases with temperature And increase, so that the thermal shock of the furnace body can be more than doubled.

Features

High density, low porosity / Good hot strength / High refractoriness and high softness

Resistance to mechanical peeling and impact, strong corrosion resistance and low wear rate.

Application

Low cement castables are widely used in power station boilers and other thermal kilns, front and back arches, furnace roofs, and rear furnace walls. They are suitable for heat treatment furnaces, various heating furnaces, shaft kilns, machinery, iron blast furnace tapholes, Ladle, ladle, etc.

Physical And Chemical Indicators

Brand/Properties

MLC-45

MLC-55

MLC-60

LC-75

LC-80

LC-85

LC-95

Application Limit Temp ℃

1580

1600

1650

1650

1700

1750

1800

Bulk Density (g/cm3)

2.4

2.5

2.55

2.55

2.6

2.7

3

Water Required for Casting (%)

5-7

5-7

5-7

7-9

7-9

6-8

6-7

Max grain size (mm)

6

6

6

6

6

6

6

CCS/MOR (MPa)

110℃x24h

80/12

90/12

100/13

65/9

70/10

80/11

90/13

1,100℃x3h

90/13

100/14

110/14

75/10

80/11

90/12

95/14

1,400℃x3h

120/14

 130/14

150/15

80/11

85/12

100/13

110/15

Chemical Analysis(%)

Al2O3

45

55

60

75

80

85

95

CaO

2-3

2-3

2-3

2-3

2-3

2-3

2-3

Fe2O3

1.5

1.5

1.5

2.4

2

1.8

1.5


  • Previous:
  • Next:

  • 1.Raw material quality control including physical and chemical testing.

    2.crushing and grinding of bulk raw materials.

    3.Packing after quality testing.

    Packaging  according to safety sea-exporting packing Standard

    Dispatch : loading the finished packing material at factory by container Door toDoor

    By 25kg kraft paper bags+sea fumigated wooden pallets