The magnesium oxide content of magnesia brick is 90%-98%. Magnesia brick has good fire resistance and corrosion resistance. It uses magnesium oxide or fused magnesia as raw materials and is fired at a high temperature of 15501600°C. It is the firing of high purity products. The temperature is above 1750℃. They are corrosion resistant and are widely used in various high temperature furnaces.


Product Detail

PRODUCTIVE PROCESS

PACKING AND SHIPPING

Product Tags

Description


The magnesium oxide content of magnesia brick is 90%-98%. Magnesia brick has good fire resistance and corrosion resistance. It uses magnesium oxide or fused magnesia as raw materials and is fired at a high temperature of 15501600°C. It is the firing of high purity products. The temperature is above 1750℃. They are corrosion resistant and are widely used in various high temperature furnaces.

Magnesia brick has the advantages of strong alkali corrosion resistance, strong erosion resistance, good thermal stability, high compressive strength, and high load softening temperature.

The refractoriness of magnesia bricks can reach more than 2000 ℃, and its load softening temperature varies greatly with the melting point of the cemented phase and the number of liquid phases produced at high temperatures. Generally, the starting temperature of load softening of magnesia bricks is between 1520 and 1600℃, while high-purity magnesia bricks can reach 1800℃.

Features

Higher temperature resistance and good refractoriness / Excellent resistance to alkaline erosion

Strong erosion resistance / Good thermal stability

High compressive strength / High load softening temperature

Application

Magnesia bricks are widely used in metallurgy (electric furnaces, converters, mixing furnaces), non-ferrous metals (smelting furnaces), high-temperature tunnel kilns, sintered magnesia kilns, building materials (cement rotary kilns, glass melting kilns, new lime kilns), steel rolling (soaking) Furnace, heating furnace) etc.

Physical And Chemical Indicators

Brand / Properties

MD92

MD95

MD97

MD98

Bulk Density (g/cm3)

2.90

2.95

3.00

3.00

@0.2MPa Refractoriness

Under Load (℃)

1550

1650

1700

1700

Apparent Porosity (%)

18

16

15

15

Cold Crushing Strength (MPa)

55

60

70

80

Thermal Shock resistance air cool  

10

10

10

10

Chemical Composition (%)

MgO

92

95

97

97.5

CaO

2.5

2.0

1.6

1.2

SiO2

3.5

2.5

1.2

0.6

Main Applications

Lime Kiln Cement Kiln
Glass melting Tank

Electric Arc Furnace

Chamber Combustor
Nonferrous Metal Furnace
Various high-temp Furnace

Productive Process

1.Raw material quality control including physical and chemical testing.
2.Crushing and grinding of bulk raw materials.
3. According to customer data sheet required to mixing Raw Material.
Pressing or shaping the green brick depend on different raw material and brick shape.
4.Dry the bricks at dryer kiln.
5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
6.The quality control department will inspect the finished refractory bricks random.

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor   
By sea fumigated wooden pallet + plastic belt  + plastic film wrap.


  • Previous:
  • Next:

  • 1.Raw material quality control including physical and chemical testing.           
    2.Crushing and grinding of bulk raw materials.
    3. According to customer data sheet required to mixing Raw Material.
    Pressing or shaping the green brick depend on different raw material and brick shape.
    4.Dry the bricks at dryer kiln.
    5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
    6.The quality control department will inspect the finished refractory bricks random.

    Packaging  according to safety sea-exporting packing Standard
    Dispatch : loading the finished packing material at factory by container Door toDoor   
    By sea fumigated wooden pallet + plastic belt  + plastic film wrap.

  • Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.