Our advantages are reduced prices,dynamic product sales workforce,specialized QC,solid factories,superior quality services for Castable Refractory Cement Australia, Andalusite Chiastolite, Mullite, Welcome you to join us together to make your business easier. We are always your best partner when you want to have your own business.
PriceList for Alumina Refractory Bricks - Zircon Nozzle – Topower Detail:

Description

Zircon nozzle is made of high-temperature refractory materials, and can also be used to connect the process, which plays a great role in controlling the flow of molten steel. The zirconium sizing nozzle has good shock and heat resistance, very high stability, and has a certain anti-corrosion function. The zirconium sizing nozzle can effectively ensure the stability of molten steel inflow and ensure the normal processing of the processing procedure.

The zirconium sizing nozzle can improve the stability of the process. Because it is manufactured at high temperature and high pressure, different schemes can be made according to the different needs of users, so it can not only ensure the normal progress of the process, but also improve the production efficiency.

The sizing nozzle is mainly used for billet continuous casting, and it is installed at the bottom of the tundish. In use, it is required to not expand or be corroded under the conditions of strong erosion and erosion of molten steel in order to stabilize the steel flow and control the continuous casting to proceed stably. There are three types of traditional sizing nozzles: inlaid, composite and integral. The so-called inlaid sizing nozzle is a zirconia ceramic refractory material with excellent performance for the part of the inner layer that contacts the molten steel. The inner and outer refractory materials are bonded together with a binder or fire mud, that is, the excellent refractory of the inner layer The material is embedded in the jacket. This sizing nozzle is very cost-effective, so it has been widely used.

The tundish inlaid sizing nozzle has obvious characteristics such as corrosion resistance, erosion resistance, and long continuous casting life.

Features

Has good anti-scouring and erosion resistance performance,

Good thermal shock stability, no explosion when used,

Long service life, use time can reach more than 20h.

Application

Mainly used for continuous casting of tundish billets, blooms, rectangular billets and small slabs for pouring steel.

Physical And Chemical Indicators

Brand
Properties

Core

External Case

ChemicalAnalysis(%)

ZrO₂

94

Al2O₃

70

Apparent Porosity (%)

22

25

Bulk Density (g/cm3)

4.5

2.4

Cold Crushing Strength (MPa)

50

25

Thermal Shock Resistance
       water cool(times)

5

Main Applications

Tundish


Product detail pictures:

PriceList for Alumina Refractory Bricks - Zircon Nozzle – Topower detail pictures

PriceList for Alumina Refractory Bricks - Zircon Nozzle – Topower detail pictures

PriceList for Alumina Refractory Bricks - Zircon Nozzle – Topower detail pictures


Related Product Guide:

Using a full scientific good quality administration system, very good quality and superior faith, we win good standing and occupied this discipline for PriceList for Alumina Refractory Bricks - Zircon Nozzle – Topower , The product will supply to all over the world, such as: Peru, Gambia, Burundi, To achieve reciprocal advantages, our company is widely boosting our tactics of globalization in terms of communication with overseas customers, fast delivery, the best quality and long-term cooperation. Our company upholds the spirit of "innovation, harmony, team work and sharing, trails, pragmatic progress". Give us a chance and we'll prove our capability. With your kind help, we believe that we can create a bright future with you together.
  • The supplier abide the theory of "quality the basic, trust the first and management the advanced" so that they can ensure a reliable product quality and stable customers.
    5 Stars By Joanne from Azerbaijan - 2018.05.15 10:52
    Customer service staff and sales man are very patience and they all good at English, product's arrival is also very timely, a good supplier.
    5 Stars By Matthew Tobias from Indonesia - 2017.12.02 14:11
    Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.