Refractory Mortar

Refractory Mortar

Short Description:

Refractory mortar consists of refractory powder, binder and admixture. Almost all refractory raw materials can be made into powder used to prepare refractory mortar. The ordinary refractory clay made by adding refractory clinker powder and an appropriate amount of plastic clay as a binder and plasticizer is called ordinary refractory clay, which has low strength at room temperature, and high strength is formed by ceramic bonding at high temperatures. The chemically bonded refractory clay, which uses hydraulic, air-hardened or thermosetting bonding materials as the bonding agent, produces a certain chemical reaction and hardens before it is lower than the ceramic bonding temperature.


Product Detail

Productive Process

Packing And Shipping

Product Tags

Description

Refractory mortar consists of refractory powder, binder and admixture. Almost all refractory raw materials can be made into powder used to prepare refractory mortar. The ordinary refractory clay made by adding refractory clinker powder and an appropriate amount of plastic clay as a binder and plasticizer is called ordinary refractory clay, which has low strength at room temperature, and high strength is formed by ceramic bonding at high temperatures. The chemically bonded refractory clay, which uses hydraulic, air-hardened or thermosetting bonding materials as the bonding agent, produces a certain chemical reaction and hardens before it is lower than the ceramic bonding temperature.

The particle size of refractory mortar varies according to the requirements of use, and its limit particle size is generally less than 1mm, and some are less than 0.5mm or finer.

The material of refractory mortar should be considered consistent with the material of refractory products of masonry. In addition to being used as a jointing material, refractory mortar can also be used as a protective coating for the lining by painting or spraying.

Features

Good plasticity and convenient construction / High bonding strength, strong corrosion resistance

High refractoriness, up to 1650℃±50℃ / Good slag resistance / Heat exfoliation

Application

Refractory mortar is mainly used in coke ovens, glass furnaces, blast furnace hot blast furnaces, and other industrial furnaces. The applied industries are: metallurgy, building materials, machinery, petrochemicals, glass, boilers, electric power, steel, cement, etc.

Physical And Chemical Indicators

Properties/Brand

Alumina

Clay

Insulating

MA-39

MA-38

MA-37

MA-36

MA-35

MA-34

MA-33

MA-32

MA-31

MI-1

MI-2

MI-3

Refractoriness (SK)

39

38

37

36

35

34

33

32

31

-

-

-

Chemical Composition (%)

Al2O3

80

72

62

55

45

43

40

35

30

-

-

-

SiO2

10

18

28

34

45

47

50

55

60

-

-

-

Grain Size (%) 

-1.00M

100

100

100

100

100

100

100

100

100

100

100

100

-0.074M

55

50

40

40

40

45

45

45

45

30

30

30

Bonding strength (kg/m3)

105 ℃x24hrs

15

15

15

15

15

10

10

15

15

5

5

5

1000 ℃x3hrs

15

15

20

20

20

15

15

15

15

15

6

6

1400 ℃x3hrs

30

30

35

35

35

-

-

-

-

-

-

-

Bonding Time(min)

1~3

1~3

1~3

Main Applications

Alumina & Insulating brick joint

Clay &Insulating brick joint

Insulating brick


  • Previous:
  • Next:

  • 1.Raw material quality control including physical and chemical testing.

    2.crushing and grinding of bulk raw materials.

    3.Packing after quality testing.

    Packaging  according to safety sea-exporting packing Standard

    Dispatch : loading the finished packing material at factory by container Door toDoor

    By 25kg kraft paper bags+sea fumigated wooden pallets