Acid resistant brick has high alkali resistance, bibulous rate is low, not easy oxidation at room temperature, not easily be medium pollution, such as performance, except hydrofluoric acid and thermal phosphoric acid in chloride brine temperature, hydrochloric acid, sulfuric acid, nitric acid and other acids and alkali at room temperature for any concentration of classes, have excellent corrosion resistant. The production of Topower acid resistant brick needs to choose high quality raw materials and adopt scientific production technology to ensure its quality and performance meet the requirements.

 

Features

 

Acid resistant brick has the advantages of high acid resistance, good stability, wear resistance and impact resistance.

Acid brick

 

Physical And Chemical Indicators

 

Acid resistant brick is widely used in petroleum, chemical industry, metallurgy, electric power, chemical fiber, paper making, pharmaceutical, chemical fertilizer, food, dairy industry, juice, electroplating room and tower, pool, tank, tank and other anti-corrosion engineering, and in the underground sewage channel and open ground and other working places can play its corrosion resistance.

 

Productive Process

1.Raw material quality control including physical and chemical testing.           
2.Crushing and grinding of bulk raw materials.
3. According to customer data sheet required to mixing Raw Material.
Pressing or shaping the green brick depend on different raw material and brick shape.
4.Dry the bricks at dryer kiln.
5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
6.The quality control department will inspect the finished refractory bricks random.

product-750-487

 

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor   
By sea fumigated wooden pallet + plastic belt  + plastic film wrap.

product-750-591

 

Hot Tags: acid resistant brick, China acid resistant brick manufacturers, suppliers, factory, mullite bricks for glass furnace, coke oven industrial silica brick, refractory fire acid proof bricks, yellow clay refractory brick, Zero Thermal Expansion Refractory Silica Bricks, mullite brick for heating furnace lining

Send Inquiry

whatsapp

Phone

E-mail

Inquiry