Alumina crucibles are made of high-purity alumina (Al2O3>99.5%) and are divided into boat type and can type. They can be used for sintering of chemicals, manufacturing of metals, preparation of ceramic materials, etc. The working temperature can reach 1750℃.
MOQ<5TONS
Send Inquiry
Product Introduction
Products Description

 

Alumina crucibles are divided into arc alumina crucibles, square alumina crucibles, alumina corundum ark rectangular alumina ceramic crucibles, straight alumina crucibles and various special-shaped ceramic crucibles.

 

crucible 2

 

Products Features

 

Characteristics of crucible:
1.Highpurity:AI203>98%, good chemical corrosion resistance.
2.Good temperature resistance,long-termtrial at1600℃ and short-termat1800℃.
3.It has good resistance to sudden cold and heat,and is not easy to explode.
4.The injection molding density is high,and the high-purity alumina crucible is 99%.
 
 
The specifications of alumina ceramic crucible are:
5ml10ml 15ml 20ml 25ml 30ml,50ml,100ml,150ml,200ml,5000ml,etc,
Can process customized irregular parts.

 

crucible

 

Products Applications

 

1.Evaporation,concentration or crystallization of solution
2. Burning of solid substances

 

Physical and Chemical Indicators

 

Items

cordierite sagger

mullite sagger

corundum-mullite sagger

Bulk density(g/cm3)

2.00

2.60

2.70

Apparent porosity(%)

28.0

20.0

25.0

Room Temperature Flexural Strength(MPA)

8.00

9.50

14.0

High Temperature Flexural Strength(MPA/1400℃)

6.00

7.00

11.0

The content of Al2O3(%)

40

68.0

81.0

The content of SiO2(%)

50.0

30.0

15.0

The content of MgO(%)

5

0

0

The content of Fe2O3(%)

<1.00

<0.60

<0.60

 

Precautions for using alumina crucibles:

 

When solids need to be heated with a high fire, use a alumina ceramic crucible. When using an alumina crucible, the crucible cover is usually placed obliquely on the crucible to prevent the heated object from jumping out and to allow air to flow in and out freely for possible oxidation reactions. Because the bottom of the crucible is very small, it usually needs to be placed on a clay tripod to be directly heated by fire. The crucible can be placed upright or obliquely on the iron tripod, and can be arranged by yourself according to the needs of the experiment.

After the alumina crucible is heated, it should not be placed on a cold metal table immediately to prevent it from breaking due to rapid cooling. It should not be placed on a wooden table immediately to prevent scalding the table or causing a fire. The correct way is to leave it on the iron tripod to cool naturally, or place it on an asbestos net to cool slowly. Please use crucible tongs to take the crucible.

Hot Tags: alumina ceramic crucible, China alumina ceramic crucible manufacturers, suppliers, factory, conventional shaped fire clay brick, Zero Expansion Silica Brick, lightweight insulating castable, refractory materials, Ceramic Ball, Tundish Nozzle

Send Inquiry

whatsapp

Phone

E-mail

Inquiry