Soluble Fiber Blanket

Soluble Fiber Blanket

Short Description:

Soluble fiber blanket, compared with traditional inorganic fiber materials, the non-fibrous material content is significantly reduced, which can increase the fiber content by 20%, and the fiber distribution is more reasonable and uniform, ensuring that the product has a lower thermal conductivity; the fiber diameter is thinner and the hand feels more It is soft and can reduce the irritation to the skin of people during the use of the product. Because it has enough solubility in human body fluids to make it stay in the human body for a short time, it will not cause damage to human health, at least it will reduce the damage to human health to a minimum, so it is called soluble fiber.


Product Detail

Productive Process

PACKING AND SHIPPING

Product Tags

Description


Soluble fiber blanket, compared with traditional inorganic fiber materials, the non-fibrous material content is significantly reduced, which can increase the fiber content by 20%, and the fiber distribution is more reasonable and uniform, ensuring that the product has a lower thermal conductivity; the fiber diameter is thinner and the hand feels more It is soft and can reduce the irritation to the skin of people during the use of the product. Because it has enough solubility in human body fluids to make it stay in the human body for a short time, it will not cause damage to human health, at least it will reduce the damage to human health to a minimum, so it is called soluble fiber.

Features

Its thermal conductivity is low, and the product volume is small;

It has the advantages of hydrophobicity, long service life and convenient construction;

It can significantly improve the utilization rate of heat energy, reduce production energy consumption and costs, and create higher value for customers.

Application

High temperature insulation for steel, petrochemical and electric power;

Industrial kiln, heating device wall lining, backing insulation;

High temperature equipment and pipeline insulation;

Heat insulation and fire prevention of electrical components;

Physical And Chemical Indicators

 Brand Properties 

Soluble fiber blanket

   Specification Temp. (℃)

1260

 Working Temp. (℃)

1100

 Bulk Density (kg/m3)

64

96

128

Linear Shrinkage after Heating

(%)@24 hours

-2.5

(1000℃)

Tensile strength (MPa)

0.03

0.04

0.05

 Fiber Diameter(μm)

3.5

Shot content (%)

12

  Thermal Conductivity (w/m.k)

200℃

0.073

0.065

0.048

400℃

0.105

0.098

0.087

800℃

0.176

0.153

0.135

Chemical

Composition (%)

SiO2

55-65%

CaO

23-35%

MgO

5-10%

Productive Process

1.Raw material quality control including physical and chemical testing.

2.crushing and grinding of bulk raw materials.

3.Packing after quality testing.

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By hard paper carton(Outside)+plastic bags(inside).


  • Previous:
  • Next:

  • 1.Raw material quality control including physical and chemical testing.           
    2.Crushing and grinding of bulk raw materials.
    3. According to customer data sheet required to mixing Raw Material.
    Pressing or shaping the green brick depend on different raw material and brick shape.
    4.Dry the bricks at dryer kiln.
    5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
    6.The quality control department will inspect the finished refractory bricks random.

    Packaging  according to safety sea-exporting packing Standard
    Dispatch : loading the finished packing material at factory by container Door toDoor   
    By sea fumigated wooden pallet + plastic belt  + plastic film wrap.

    Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.