Wholesale Ceramic Fiber Insulation Blanket - Rockwool Blanket – Topower Detail:

Description

Rock wool blanket has good thermal insulation performance, convenient construction and installation, significant energy-saving effect, and high cost performance; rock wool blanket is a kind of thermal insulation material with low thermal conductivity. It is suitable for large and medium-diameter pipelines; medium and small storage tanks and equipment with small curved surfaces or irregular surfaces, building air-conditioning pipe insulation and anti-dew, and sound absorption and insulation of walls.

Rock wool blanket products use basalt as the raw material, which has good non-combustibility, and the melting point is above 1000℃. It is particularly effective in heat insulation and fire prevention, reducing or absorbing noise.

Features

Non-flammable / Fire prevention / Pest control

Asbestos free / Stable chemical properties

No effect on human body and environment / Easy to handle and transport / Low maintenance cost

Application

Rock wool blankets are suitable for heat preservation, heat insulation, sound insulation and noise reduction of large pipelines, containers, storage tanks, boilers, and conveying pipelines. The rock wool blanket has a metal wire mesh with a single-sided reinforcement mesh, and its firm binding force ensures that the rock wool will not be torn or damaged.

Affixed with aluminum foil can better meet the needs of heat insulation and water vapor barrier for HVAC ducts, heating and cooling water pipes, and for building heat insulation. Make the room warm in winter and cool in summer, and comfortable in four seasons

Physical And Chemical Indicators

Brand / Properties

Soluble fiber blanket

   Specification Temp. (℃)

1260

 Working Temp. (℃)

1100

 Bulk Density (kg/m3)

64

96

128

Linear Shrinkage after Heating

(%)@24 hours

-2.5

(1000℃)

Tensile strength (MPa)

0.03

0.04

0.05

 Fiber Diameter(μm)

3.5

Shot content (%)

12

  Thermal Conductivity (w/m.k)

200℃

0.073

0.065

0.048

400℃

0.105

0.098

0.087

800℃

0.176

0.153

0.135

Chemical

Composition (%)

SiO2

55-65%

CaO

23-35%

MgO

5-10%

Productive Process

1.Raw material quality control including physical and chemical testing.

Put the selected raw materials in the furnace for high temperature spinning.

2.Needle with the needling machine.

3.Cut the board into the size required by the customer.

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By hard paper carton(Outside)+plastic bags(inside).


Product detail pictures:

Wholesale Ceramic Fiber Insulation Blanket - Rockwool Blanket – Topower detail pictures

Wholesale Ceramic Fiber Insulation Blanket - Rockwool Blanket – Topower detail pictures

Wholesale Ceramic Fiber Insulation Blanket - Rockwool Blanket – Topower detail pictures


Related Product Guide:

With dependable high-quality method, fantastic standing and ideal purchaser assistance, the series of products produced by our firm are exported to many countries and regions for Wholesale Ceramic Fiber Insulation Blanket - Rockwool Blanket – Topower , The product will supply to all over the world, such as: kazan, Mexico, Egypt, By continuous innovation, we will present you with more valuable items and services, and also make a contribution for the development of the automobile industry at home and abroad. Both domestic and foreign merchants are strongly welcomed to join us to grow together.
  • The sales person is professional and responsible, warm and polite, we had a pleasant conversation and no language barriers on communication.
    5 Stars By Margaret from Romania - 2018.10.01 14:14
    It is a very good, very rare business partners, looking forward to the next more perfect cooperation!
    5 Stars By Samantha from Kuwait - 2017.04.28 15:45
    Write your message here and send it to us

    PRODUCT CATEGORIES

    Focus on providing mong pu solutions for 5 years.