Zircon Nozzle

Short Description:

Zircon nozzle is made of high-temperature refractory materials, and can also be used to connect the process, which plays a great role in controlling the flow of molten steel. The zirconium sizing nozzle has good shock and heat resistance, very high stability, and has a certain anti-corrosion function. The zirconium sizing nozzle can effectively ensure the stability of molten steel inflow and ensure the normal processing of the processing procedure.

The zirconium sizing nozzle can improve the stability of the process. Because it is manufactured at high temperature and high pressure, different schemes can be made according to the different needs of users, so it can not only ensure the normal progress of the process, but also improve the production efficiency.


Product Detail

Product Tags

Description

Zircon nozzle is made of high-temperature refractory materials, and can also be used to connect the process, which plays a great role in controlling the flow of molten steel. The zirconium sizing nozzle has good shock and heat resistance, very high stability, and has a certain anti-corrosion function. The zirconium sizing nozzle can effectively ensure the stability of molten steel inflow and ensure the normal processing of the processing procedure.

The zirconium sizing nozzle can improve the stability of the process. Because it is manufactured at high temperature and high pressure, different schemes can be made according to the different needs of users, so it can not only ensure the normal progress of the process, but also improve the production efficiency.

The sizing nozzle is mainly used for billet continuous casting, and it is installed at the bottom of the tundish. In use, it is required to not expand or be corroded under the conditions of strong erosion and erosion of molten steel in order to stabilize the steel flow and control the continuous casting to proceed stably. There are three types of traditional sizing nozzles: inlaid, composite and integral. The so-called inlaid sizing nozzle is a zirconia ceramic refractory material with excellent performance for the part of the inner layer that contacts the molten steel. The inner and outer refractory materials are bonded together with a binder or fire mud, that is, the excellent refractory of the inner layer The material is embedded in the jacket. This sizing nozzle is very cost-effective, so it has been widely used.

The tundish inlaid sizing nozzle has obvious characteristics such as corrosion resistance, erosion resistance, and long continuous casting life.

Features

Has good anti-scouring and erosion resistance performance,

Good thermal shock stability, no explosion when used,

Long service life, use time can reach more than 20h.

Application

Mainly used for continuous casting of tundish billets, blooms, rectangular billets and small slabs for pouring steel.

Physical And Chemical Indicators

Brand
Properties

Core

External Case

ChemicalAnalysis(%)

ZrO₂

94

--

Al2O₃

--

70

Apparent Porosity (%)

22

25

Bulk Density (g/cm3)

4.5

2.4

Cold Crushing Strength (MPa)

50

25

Thermal Shock Resistance
       water cooltimes

5

--

Main Applications

Tundish


  • Previous: