Turkey Customer Orders 20 Tons Topower Ceramic Fiber Blanket For Furnace Insulation Application

This recent 20-ton orderfrom a leading Turkish furnace manufacturer highlights the growing preference for Topower's high-performance ceramic fiber blankets in extreme heat applications. The customer specifically required 1260°C-grade blankets with low shot content (<15%) for their aluminum melting furnaces, emphasizing the need for longevity, thermal shock resistance, and energy savings-key concerns for industrial buyers in the region.

Why Turkish Buyers Choose Topower Ceramic Fiber insulation Blankets?

ceramic fiber blanket


1. Superior Thermal Performance
temperature Resistance: Continuous service up to 1260°C (2300°F), with short-term exposure to 1400°C (2552°F)
Low Thermal Conductivity:0.12 W/m·K at 600°C, reducing furnace heat loss by 25-30%
-Energy Savings: 40% faster heat-up/cool-down cycles compared to traditional refractory linings
2. Durability & Chemical Resistance
Low Biopersistent Fiber (Bio-Soluble): Complies with EU REACH & Turkey's occupational safety regulations
Acid/Alkali Resistance: Withstands corrosive furnace atmospheres (pH 2-12)
Long Service Life: 3-5 years in aluminum furnaces vs. 1-2 years for conventional insulation
3. Customization for Turkish Market Needs
Density Options: ceramic fiber blankets 96 kg/m³ (standard) to 160 kg/m³ (high mechanical strength)
Thickness: 25mm, 50mm, 75mm (cut-to-size for furnace lining optimization)
Reinforcement: Optional stainless steel wire mesh for high-velocity gas environments .

Q1: How does ceramic fiber compare to rock wool for furnace insulation?
A: Ceramic fiber offers **2x higher temperature resistance (1260°C vs. 650°C) and 50% better energy efficiency, though rock wool may be preferred for low-cost, low-heat applications.
Q2: What's the lead time for bulk orders to Turkey?
A: 15-20 days for standard grades (20-ton orders), including Istanbul/Izmir port clearance support.
Q3: Are these blankets compliant with Turkish safety standards?
A: Yes, our products meet TSE 1260 & EU Regulation 1272/2013 for hazardous substances.
Q4: How to install ceramic fiber blankets in high-vibration furnaces?
A: We recommend **anchoring with ceramic fasteners + high-temp adhesive-installation guides provided.
Q5: What's the cost difference vs. traditional firebricks?
A: 30-40% lower initial cost + 50% reduced energy expenses due to superior insulation.