Ceramic Fiber Textiles
video

Ceramic Fiber Textiles

Ceramic Fiber Textiles are a kind of high-temperature fiber products composed of high purity alumina and silicate fibers. Mainly includes ceramic fiber blanket, yarn, tape and plate and other different forms, widely used in thermal equipment and high temperature pipe insulation, insulation and sealing fields.
MOQ: 50 rolls
Send Inquiry
Product Introduction
Description

 

Ceramic fiber textiles use different textile processes and equipment are used to woven into cloth, belt, rope and other products, which have good thermal insulation performance, which is superior to traditional ceramic fiber products such as high strength, mechanical vibration resistance and impact resistance. Industrial refractory fibre is made from ceramic fibre, E-Glass Fibre,vycor fibre, PANOF, etc material, the products include yarn, cloth, tape, twisted rope, packing, tube, Coated Fabric and other kinds of tech textiles. Widely used in heat insulation sealing etc

 

Features

 

The advantages of ceramic fiber textiles:

High temperature resistance, low thermal conductivity, thermal shock resistance, low heat capacity;

Excellent high temperature insulation performance and long service life;

It has the ability to resist the corrosion of non-ferrous metals such as aluminum and zinc;

Has good low temperature and high temperature strength;

Non-toxic, harmless, and has no adverse effects on the environment;

 

Application

 

Ceramic fiber textiles can be widely used in the chemical industry, electric power, paper making, food, pharmaceutical and other industries, boiler doors, high temperature, high pressure machines, pumps, valve sealing. It is suitable for clean fluid or slurry, salt water, emulsion, grease, hydrocarbon, solvent, pulp and other media.

 

Physical And Chemical Indicators

 

Brand
     Properties

Bio-Soluble fiber rope/cloth/tap/yarn

Ceramic fiber rope/cloth/tap/yarn

GF-Rope/Cloth/

Tape/Yarn

SS-Rope/Cloth/

Tape/Yarn

GF-Rope/Cloth/

Tape/Yarn

SS-Rope/Cloth/

Tape/Yarn

Specification Temp. (℃)

1260

Working Temp. (℃)

500-600

1100

500-600

1100

Bulk Density (kg/m3)

500

Organic matter (%)

15

Moisture Content(%)

1

Chemical Composition(%)

SiO2

55-65

51

CaO

23-35

--

MgO

On May 10

--

Al2O3

--

45

Fe2O3

--

0.8

 

Productive Process

 

1.Raw material quality control including physical and chemical testing.

2.Crushing and grinding of bulk raw materials.

3.Packing after quality testing.

 

product-750-485

 

Packing And Shipping

Packaging according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By 25kg kraft paper bags+sea fumigated wooden pallets

product-750-549