Ceramic Fiber Bulk
MOQ: 500 kg
Description
Ceramic fiber bulk is a high-temperature refractory fiber made of high-purity raw materials through high-temperature melting, using blowing or spinning technology. The fiber has good chemical stability and can resist the erosion of most aggressive chemicals. Even if the finished product is wetted by oil, water or steam, its physical properties such as temperature resistance and heat insulation will not change. Fiber cotton can be further processed into fiber blanket, felt, board, paper, cloth, rope and other products.
Features

Ceramic fiber bulk has good high temperature resistance and chemical stability, can be used at high temperature for a long time without damage. And also has the following characteristics:
Light weight, anti-oxidation
Low thermal conductivity, good flexibility
White, precise size, easy to cut and install, convenient
Does not contain any adhesives, can be used for a long time in neutral and oxidizing environments
Low heat capacity, low thermal conductivity, high refractoriness and high heat sensitivity
Excellent resistance to wind erosion and mechanical shock
Excellent sound absorption and fire resistance
Stable density and performance
Application
Ceramic fiber bulk is commonly used in industrial heating equipment, aerospace equipment, automotive manufacturing and other applications requiring high temperature protection.
Industrial kilns, boiler linings, lining insulation, refractory insulation
Thermal insulation of steam engines, gas engines and other thermal equipment
Flexible insulating material for high temperature pipeline; high temperature gasket; high temperature filtration
Thermal reactor insulation
Fire protection of various industrial equipment, heat insulation and fire protection of electrical components
Thermal insulation materials for incineration equipment
Materials for modules, folding blocks and veneer blocks
Thermal insulation of investment castings

Physical And Chemical Indicators
|
Brand Properties |
STD BULK |
HP BULK |
HZ BULK |
PC BULK |
|
|
(%) Chemical Composition |
Al2O3 |
43 |
44 |
34 |
71-73 |
|
|
SiO2 |
54 |
55 |
50 |
- |
|
|
Fe2O3 |
1.0 |
0.5 |
0.5 |
0.2 |
|
|
ZrO2 |
- |
- |
15 |
- |
|
Specification Temp. (℃) |
1260 |
1260 |
1430 |
1600 |
|
|
Shot content (%) |
15 |
15 |
12 |
1 |
|
|
Fiber Diameter(μm) |
3-5 |
4-6 |
|||
Productive Process
1.Raw material quality control including physical and chemical testing.
2.crushing and grinding of bulk raw materials.
3.Packing after quality testing.

Packing And Shipping
1.Raw material quality control including physical and chemical testing.
2.crushing and grinding of bulk raw materials.
3.Packing after quality testing.