Soluble Fiber Blanket
video

Soluble Fiber Blanket

Soluble fiber blanket, compared with traditional inorganic fiber materials, the non-fibrous material content is significantly reduced, which can increase the fiber content by 20%.
MOQ: 50 rolls
Send Inquiry
Product Introduction
Description

The fiber diameter of soluble fiber blanket is thinner and the hand feels more It is soft and can reduce the irritation to the skin of people during the use of the product. Because it has enough solubility in human body fluids to make it stay in the human body for a short time, it will not cause damage to human health, at least it will reduce the damage to human health to a minimum, so it is called soluble fiber. And the fiber distribution is more reasonable and uniform, ensuring that the product has a lower thermal conductivity.

 

Features

 

The thermal conductivity of soluble fiber blanket is low, and the product volume is small; It has the advantages of hydrophobicity, long service life and convenient construction. It can significantly improve the utilization rate of heat energy, reduce production energy consumption and costs, and create higher value for customers.

 

ceramic fiber blanket

 

 

Application

 

High temperature insulation for steel, petrochemical and electric power;

Industrial kiln, heating device wall lining, backing insulation;

High temperature equipment and pipeline insulation;

Heat insulation and fire prevention of electrical components;

 

Physical And Chemical Indicators

 

                               Properties

Soluble Fiber Blanket

Specification Temp. (℃)

1100

1300

Bulk Density (kg/m3)

64

96

128

96

128

@24

Linear Shrinkage after Heating

1100℃x24h≤1.0

1260℃x24h≤3.0

Tensile strength (MPa)

0.03

0.05

0.07

0.05

0.07

Shot content (%)

≤12

≤12

(w/m.k) Thermal Conductivity

200℃

0.06

0.05

0.05

0.05

0.04

 

400℃

0.11

0.09

0.08

0.10

0.08

 

600℃

0.17

0.13

0.12

0.18

0.14

 

800℃

0.28

0.20

0.17

0.30

0.22

 

1000℃

0.40

0.28

0.25

0.46

0.33

 

1200℃

-

-

-

0.68

0.46

 

Chemical

Composition

SiO2

62-68

≥70

 

CaO

26-32

-

 

MgO

4-7

-

 

CaO+MgO

-

≥20

Size(mm)

 LENGTH*WIDTH*THICKNESS
7200*610/1220*25,3600*610/1220*50,4800*610/1220*38
7200*610/1220*6,14400*610/1220*12.5,28800*610/1220*6.38

 

Productive Process

 

1.Raw material quality control including physical and chemical testing.

2.crushing and grinding of bulk raw materials.

3.Packing after quality testing.

bio solube fiber blanket process

 

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By hard paper carton(Outside)+plastic bags(inside).

product-750-549

 

Hot Tags: soluble fiber blanket, China soluble fiber blanket manufacturers, suppliers, factory, Silicone Mullite Refractory Brick, Phlogolite Mica Plate, Ceramic Fiber Rope, Ceramic Fibre Cotton, Chrome Ceramic Fiber Blanket for furnace lnsulation, Aerogel insulation felt

Send Inquiry

whatsapp

Phone

E-mail

Inquiry