What is ceramic fiber paper?

Ceramic Papers are made of high purity refractory fibers and are intended for high temperature insulation. Advanced manufacturing procedures enable consistent fiber distribution as well as tight control over thickness and density. Ceramic Fiber Papers are utilized to tackle a wide range of heat-related issues and have good chemical stability, withstanding most corrosive substances. Ceramic Paper is classified according to their thickness, density, fiber index, and chemistry. Ceramic Fiber Papers are subjected to numerous industry standards tests.

 

Features

Ceramic fiber Paper has a lightweight, homogeneous structure, and low thermal conductivity, making it an ideal solution for high temperature insulation, chemical corrosion resistance, and thermal shock resistance. Ceramic Paper has a wide range of refractory and sealing uses. It has low thermal conductivity, flexibility, and good handling strength.

 

Application

Ceramic paper can be used in a variety of refractory and sealing applications. Such as separating the plane in the refractory lining, using in the spare lining of the metal groove and as a hot -top lining. Commercial and residential cooking and heating equipment insulation also install it.

 

product-300-224

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Physical And Chemical Indicators

 

Brand 
Properties
DK-1260 DK-1350 DK-1430
Specification Temp 1000 1100 1300
Bulk Density 200 200 200
Tensile strength 0.4
Organic matter content(%) ≤8
Thickness (mm) 0.5-10mm
Width (mm) 610mm  1220mm
Chemical Composition Al2O3 47 48 40
SiO2 52 51 15-17 ZrO2
Fe2O3 0.5 0.5 0.2
NaO2 0.2  0.2 0.2

 

Productive Process

How to make ceramic fiber paper?

1. Use spray fiber (short fiber, fine, easy to break and mixed) as the raw material of ceramic fiber paper, add a certain proportion of binding agents and fillers -level additives. Essence
2. Use a pump to enter the molding pool and stir with compressed air. Put the mold into the molding pool and use the principle of vacuum to absorb fibrous slurry to the mold. Precisely control the adsorption time, perform vacuum dehydration of fiber wet materials, remove the mold, and give people dry furnace dry for 10-24 hours.
3. The drying ceramic paper is accurately controlled by a special grinding machine and cutting machine to accurately control the size.

 