Ceramic Fiber Module
Description
The ceramic fiber module has excellent chemical stability; excellent thermal stability; excellent elasticity. The product is white in color and regular in size. It can be directly fixed on the anchor nails of the steel plate of the industrial kiln shell. After the furnace lining is built, the expansion of the ceramic fiber foldable module makes the furnace lining seamless and can compensate for the fiber furnace lining Shrink to improve the thermal insulation performance of the fiber lining, and the overall performance is good; excellent thermal stability and thermal shock resistance; It is easy to install, and the anchors are set on the cold surface of the wall lining, which can reduce the requirements for refractory anchor materials.
Features
Ceramic fiber module has a good fire-resistant and heat-insulating effect, which improves the integrity of the fire-resistant and heat-insulating kiln and promotes the progress of kiln masonry technology. And also has the following features:
Low bulk density, low thermal conductivity
Resistance to thermal shock and airflow
High mechanical strength, built-in anchors, good safety performance
The installation is simple, the furnace lining forms a seamless whole after installation, and the thermal insulation effect is good

Application
Application of ceramic fiber module:
Ceramic industry: tunnel kiln, shuttle kiln, roller kiln
Petrochemical industry: atmospheric furnace, conversion furnace, coking furnace, cracking furnace, heating furnace, flue, etc.
Iron and steel industry: ladle cover, heating furnace, annealing furnace, bell furnace, walking furnace, hot blast pipe and pipe, etc.
Environmental protection and energy saving industry: waste incinerator, RTO exhaust gas treatment furnace, SCR environmental protection catalytic furnace, etc.

Physical And Chemical Indicators
|
Brand Properties |
STD Module |
HP Module |
HZ Module |
PC Module |
|
|
(%) Chemical Composition
|
Al2O3 |
44 |
45 |
34 |
71 |
|
SiO2 |
52 |
54 |
50 |
27 |
|
|
Fe2O3+TiO2 |
1.0 |
0.5 |
0.5 |
- |
|
|
ZrO2 |
- |
- |
15 |
- |
|
|
K2O+Na2O+Fe2O3 |
1.0 |
0.2 |
0.2 |
0.2 |
|
|
Bulk Density (kg/m3) |
128-240 |
128-240 |
128-240 |
128-196 |
|
|
Specification Temp. (℃) |
1260 |
1350 |
1430 |
1600 |
|
|
(%) Linear Shrinkage after Heating |
1000℃X24h≤2.5 |
1000℃X24h≤2.5 |
1000℃X24h≤3.5 |
1400℃X24h≤1.0 |
|
|
(w/m.k) Thermal Conductivity
|
400℃ |
0.090 |
0.101 |
0.118 |
0.09 |
|
500℃ |
0.119 |
0.120 |
0.149 |
0.133 |
|
|
600℃ |
0.152 |
0.175 |
0.172 |
0.160 |
|
|
Size(mm) |
LENGTH:250-600 WIDTH:200-400 THICKNESS:200-400 |
LENGTH:100-600 WIDTH:150-300 THICKNESS:200-300 |
|||
Packing And Shipping
Packaging according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By 25kg kraft paper bags+sea fumigated wooden pallets

Hot Tags: ceramic fiber module, China ceramic fiber module manufacturers, suppliers, factory, Ceramic Fiber Bulk, Zirconium Filled Ceramic Fiber Blanket, Silica Aerogel Insulation Blanket, moisture resistant rockwool board, Zirconium containing Ceramic Fiber Blanket, 1600c chrome ceramic blanket