Ceramic Fiber Rope
video

Ceramic Fiber Rope

Ceramic fiber rope is made by spinning and weaving spun silk filament with excellent spinnability as raw materia.It is a versatile and high-performance insulation material with excellent thermal insulation properties.
Send Inquiry
Product Introduction
Description


Ceramic fiber rope has excellent heat resistance, continuous use temperature up to l260℃, excellent resistance to acid, oil and water vapor, corrosion resistance to non-ferrous molten metals such as aluminum and zinc, excellent high-temperature strength, and excellent tensile strength The strength and low thermal conductivity make the products have excellent heat insulation performance, excellent electrical insulation, non-toxic and harmless, and have no adverse effects on the environment.

 

Features

 

Here are some key features and details about creamic fiber rope:

Composition:
It is primarily composed of high-quality alumina-silica ceramic fibers. These fibers are manufactured by melting a combination of alumina and silica raw materials at high temperatures and then spinning them into fine, flexible fibers.

Temperature Resistance:
It is designed to withstand high temperatures and can typically operate in temperature ranges up to 1000°C (1832°F) or higher, depending on the specific product and application. It exhibits excellent thermal stability and retains its insulation properties even at elevated temperatures.

Thermal Insulation Properties:
Ceramic fiber rope offers exceptional thermal insulation, effectively reducing heat transfer and preventing energy loss. It has low thermal conductivity, which helps maintain temperature stability and improves energy efficiency in various applications.

Flexibility and Durability:
It is highly flexible and can be easily bent, twisted, or wrapped around complex shapes. It is available in various diameters and lengths to suit different requirements. The rope's flexibility allows for easy installation and sealing of joints, flanges, and other components in high-temperature environments.

Chemical Resistance:
Ceramic fiber insulation rope exhibits good resistance to most chemicals, including acids, alkalis, and organic solvents. This makes it suitable for applications where exposure to corrosive substances is a concern.

 

ceramic fiber rope

 

Application

 

Ceramic fiber rope can replace asbestos textiles and are widely used in fire resistance, heat insulation, fire protection, and sealing in industrial sectors such as metallurgy, chemical industry, ceramics, glass, refractory materials, ships, aviation, automobiles, machinery, electronics, building materials, light industry, etc.; friction system Motion, noise reduction, high-temperature filtration and other fields.

 

application

 

 

Physical And Chemical Indicators

 

Brand Properties Bio-Soluble fiber rope Ceramic fiber rope
GF-Rope SS-Rope GF-Rope SS-Rope
Specification Temp. (℃) 1260
Working Temp. (℃) 500-600 1100 500-600 1100
Bulk Density (kg/m3) 500
Organic matter (%) 15
Moisture Content(%) 1
Chemical Composition(%) SiO2 55-65 51
CaO 23-35 --
MgO May 10th --
Al2O3 -- 45
Fe2O3 -- 0.8
Reinforced material Glass Filament Stainless steel 304 Glass Filament Stainless steel 304
Note: Rope Dia size :(mm)6/10/12/20/25/32/38/50, Rope Shape: Round Braided Rope& Twisted Rope &Square Braided Rope

 

Hot Tags: ceramic fiber rope, China ceramic fiber rope manufacturers, suppliers, factory, Silicon Carbide Refractory Plate, Chrome Ceramic Fiber Blanket for furnace lnsulation, Silica Aerogel Insulation Blanket, mineral wool board, Soluble Fiber Board, Cordierite Mullite Kiln Car Brick

Send Inquiry

whatsapp

Phone

E-mail

Inquiry