Soluble Fiber Board
video

Soluble Fiber Board

Soluble fiber board is made of soluble fiber cotton, refractory fillers, a small amount of organic binders and inorganic binders, and has excellent thermal insulation and processing properties.
MOQ: 50 pieces
Send Inquiry
Product Introduction
Description

Soluble fiber board is mainly made of some type of fiber material through special processing, with fire resistance, fire prevention, water resistance, corrosion resistance, high temperature resistance and other characteristics, has good thermal stability, can be used in high temperature environment for a long time

 

Features

 

Environmental protection and high safety, soluble and biodegradable / Softer texture and less irritation / Lower shot content

Can resist far infrared radiation, lower thermal conductivity / Better thermal stability / Stronger chemical resistance

Good heat resistance / Low thermal conductivity, low heat capacity / Flat appearance, accurate size, easy to install and use

 

 

ceramic fiber board

 

 

Application

 

The application of soluble fiber board is as follow:

Insulation of household thermal equipment, such as thermal storage electric heaters, ovens

Civil building exterior wall insulation and elevator door fire protection

Insulation layer of various environmental protection equipment and mine life-saving equipment

Refractory layer or insulation lining of various industrial furnace equipment

Furnace door sealing, flange sealing, pipe insulation

Thermal insulation of industrial energy storage equipment

Heat insulation, sound insulation and noise reduction of automobile exhaust system

Fire and heat insulation of marine drilling platforms and ships

High temperature and heat insulation in nuclear power field

 

application

 

 

Physical And Chemical Indicators

Brand
Properties

Soluble fiber board

Specification Temp. (℃)

1100

1300

 Bulk Density (kg/m3)

300

300

(%)@24H

Linear Shrinkage after Heating

1000℃x24h≤2.0

1260℃x24h≤2.0

(MPa) Tensile Strength

0.15

0.15

 (w/m.k) Thermal Conductivity

400℃

0.08

0.07

 

600℃

0.11

0.10

 

800℃

0.12

0.11

 

1000℃

0.15

0.14

 Size(mm)

 LENGTH*WIDTH*THICKNESS
900*600*20/25/30/40/50

1000*500*20/25/30/40/50, 1000*600*20/25/30/40/50

1200*1000*20/25/30/40/50, 1200*600*20/25/30/40/50

 

Productive Process

1.Raw material quality control including physical and chemical testing.

Put the selected raw materials in the furnace for high temperature spinning.

2.Needle with the needling machine.

3.Cut the board into the size required by the customer.

 

ceramic fiber board

 

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By hard paper carton(Outside)+plastic bags(inside).

product-750-549

 

Hot Tags: soluble fiber board, China soluble fiber board manufacturers, suppliers, factory, Airgel blanket, Ceramic Fiber Textiles, Airgel insulation blanket, Vermiculite Fireproof Board, Insulation Thermal Material, Zirconia Ceramic Blanket