Glass Fiber Cloth
video

Glass Fiber Cloth

Glass Fiber Cloth has the functions of heat insulation, fire prevention and flame retardant. It absorbs a lot of heat when it is burned by the flame and can prevent the flame from passing through and isolate the air.
MOQ: 10 rolls
Send Inquiry
Product Introduction
Description

 

Glass fiber cloth is usually used as a reinforcing material in composite materials, electrical insulating materials and thermal insulation materials, circuit substrates and other fields of the national economy.

Glass fiber cloth is mostly used in hand lay-up process, and it is mainly used in ship hulls, storage tanks, cooling towers, ships, vehicles, tanks, etc. It is an ideal engineering material in the construction industry. Fiberglass cloth is mainly used in industry for: heat insulation, fire prevention and flame retardant. The material absorbs a lot of heat when it is burned by a flame and can prevent the flame from passing through and isolate the air.

 

Features

 

The glass fiber cloth has weather resistance , Non-adhesive, not easy to adhere to any substance , high insulation properties and high strength .The transmittance is 6~13%.

 

Application

 

Fiberglass cloth is widely used in wall reinforcement, external wall insulation, roof waterproofing, etc. It can also be used in the reinforcement of wall materials such as cement, plastic, asphalt, marble, mosaic, etc.

 

Physical And Chemical Indicators

Product

Glass fiber Cloth

Item

Standard

Product Code

CW1500

Wide(cm)

100.00

Weave Style

Plain

Weft Counts (ends/cm)

3.2±0.5

Warp Counts (ends/cm)

5.6±1

Breaking Strength (N/50*200)

1870*1700

Weight (g/m²)

1000±100

STD Roll (M/ roll)

30

Thinckness (mm)

1.5±0.15

L.0.1%

7~12

Working Temperature

550 ℃

 

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor   
By sea fumigated wooden pallet + plastic belt  + plastic film wrap.