Rockwool Blanket
video

Rockwool Blanket

Rockwool blanket is a kind of high-performance thermal insulation material made of asbestos as the main raw material, which has good non-combustibility, and the melting point is above 1000℃.
MOQ: 100 rolls
Send Inquiry
Product Introduction
Description


Rockwool blanket has good thermal insulation performance, convenient construction and installation, significant energy-saving effect, and high cost performance. It is suitable for large and medium-diameter pipelines; medium and small storage tanks and equipment with small curved surfaces or irregular surfaces, building air-conditioning pipe insulation and anti-dew, and sound absorption and insulation of walls.

It is particularly effective in heat insulation and fire prevention, reducing or absorbing noise.

 

Features

 

Rockwool blanket has excellent thermal insulation properties, which can effectively prevent the transfer of heat, sound and vibration. In addition, it also has good fire resistance, chemical stability and water resistance, can withstand high pressure and tensile strength, has good durability and service life. The thickness, density and size of rock wool blanket can be adjusted according to the needs, so it has a wide range of applications in various fields.

product-750-500

 

 

Application

 

Rockwool blanket is suitable for heat preservation, heat insulation, sound insulation and noise reduction of large pipelines, containers, storage tanks, boilers, and conveying pipelines. Affixed with aluminum foil can better meet the needs of heat insulation and water vapor barrier for HVAC ducts, heating and cooling water pipes, and for building heat insulation. Make the room warm in winter and cool in summer, and comfortable in four seasons

It has a metal wire mesh with a single-sided reinforcement mesh, and its firm binding force ensures that the rock wool will not be torn or damaged.

application

 

Physical And Chemical Indicators

Brand

Properties

JC-Z650

Bulk Density (kg/m3)

80-150

(°C) Maximum use temperature

750

(%)Volumetric hygroscopic rate

≤1

(%)Mass hygroscopic rate

≤1

(w/m.k) Thermal Conductivity

70℃

0.038

150℃

0.048

200℃

0.056

300℃

0.070

400℃

0.085

 

Surface burning characteristics

 Flue gas development index

≤25

 

 Flame spread index

0

Size(mm)

LENGTH*WIDTH*THICKNESS 1200*600*20/25/50/80/100MM

 

Productive Process

 

1.Raw material quality control including physical and chemical testing.

Put the selected raw materials in the furnace for high temperature spinning.

2.Needle with the needling machine.

3.Cut the Rockwool blanket into the size required by the customer.

 

Packing And Shipping

 

Packaging  according to safety sea-exporting packing standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By hard paper carton(Outside)+plastic bags(inside).

 

Hot Tags: rockwool blanket, China rockwool blanket manufacturers, suppliers, factory, High Zirconia ceramic fibre Blankets, Ceramic Fiber Rope, Ceramic Fiber Modules, Cordierite Mullite Kiln Car Brick, Silica Aerogel Insulation Blanket, Ceramic Fiber Module