Aerogel Glass Fiber Blanket
Products Description
The biggest feature of Aerogel Glass Fiber Blanket is its low density and high pore rate. Because its pore rate is very high, it can absorb a large amount of liquid and gas, and has excellent thermal insulation, fire resistance and acoustic performance. In addition, gas gel also has good chemical stability and mechanical strength.
The main component of aerogel glass fiber blanket is silicon or other oxides. The preparation methods include supercritical drying, solitary-gel method. These preparation methods can control the pore size and pores of the gas gel, thereby regulating their performance, such as adsorption, insulation, insulation, damping, filtering, etc.
Features
Light quality: The density is very low, usually only about one -third of the air, but its strength is very high. This makes gas gels an ideal material for many applications, such as aerospace, construction and medical care.
Excellent thermal insulation performance: It has excellent thermal insulation performance due to the micropore structure of gas gel. Compared with traditional thermal insulation materials, such as glass fiber and polystyrazanbenzylene, gas gel's thermal insulation performance is much better.
Good fire resistance: aerogel glass fiber blanket still maintains its structure and performance at high temperature. This makes gas gel a good refractory material that can be used for firewalls, heat insulation and fireproof coatings.
Super adsorption: The micropore structure gives it super adsorption, which can adsorb a variety of substances, including gas, moisture and solution. This makes gas gel a good adsorption agent that can be used for sewage treatment, gas separation and catalyst carrier.
Sustainable environmental protection: The preparation process is friendly to the environment, and can obtain raw materials from renewable resources. This makes gas gels an environmentally friendly and sustainable material that can achieve sustainable development in many fields.

Application
Aerogel Glass Fiber Blanket can be widely used in construction, electronics, aerospace, energy, environmental protection and other fields. At present, aerogel products on the market include insulation plates, insulation pipes, insulation felt, filters, energy storage materials, etc. In the field of construction, gas gel is mainly used in the insulation and heat insulation of walls, roofs, and floors; in the electronics field, aerogel can be used in battery diaphragm, chip packaging, etc ; In the energy field, gas gel can be used in solar absorbers, water heater insulation, etc.; In the field of environmental protection, gas gel is mainly used in exhaust gas treatment and oil and water separation.

Physical and Chemical Indicators
|
Property |
Aerogel Insulation Blanket |
|
Thermal conductivity W/(m.k) |
0.020(25℃),0.036(300℃) |
|
Maximum service temperature (℃) |
650 |
|
Density (kg/m³) |
160-240 |
|
Hydrophobicity rate (%) |
99.9 |
|
Combustion performance grade |
A |
|
Compression rebound rate (%) |
96 |
|
Permanent change rate of heating line (%) |
- 0.3 |
|
Tensile strength (kpa) |
1409 (landscape orientation),366 (portrait orientation) |
|
Surface property |
Bulk drain |
|
Colour |
White/grey blue |
|
Size(mm) |
Wide:1500±5, Thickness:5/10/15 (customizable 3/6) |
Productive Process
1. Raw material of ceramic fiber blanket has quality control including physical and chemical testing.
Put the selected raw materials in the furnace for high temperature spinning.
2. Needle with the needling machine.
3. Roll up the woven blanket.

Packing and Shipping
Packaging according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By hard paper carton(Outside)+plastic bags(inside).