Aug 20, 2021ADVANTAGES OF SINTERED BRICK TUNNEL KILN LIGHTWEIGHT MULLITE BRICK CeilingProduct characteristics: Low thermal conductivity, low heat capacity; high purity, low impurity content; high temperature resistance, direct flame contact; high strength, and ex... -
Aug 13, 2021THE INTRODUCTION OF MAGNESIA BRICKThe main crystal phase of magnesia brick is periclase, which has the typical characteristics of general alkaline refractory products, but its thermal shock resistance is poor. I... -
Aug 06, 2021【SPECIAL CEMENT】REFRACTORY CEMENTAny raw material with high-quality bauxite and high-quality lime as raw materials, mixed in a certain proportion to form an appropriate amount of raw material, after sintering, ... -
Aug 05, 2021SOME KNOWLEDGE ABOUT CORUNDUM REFRACTORY CASTABLEAmong silicon-aluminum refractory castables, refractory castables with Al₂O₃ content greater than 90% belong to corundum refractory castables. Design principles of corundum cast... -
Jul 30, 2021HOW ARE REFRACTORY BRICKS FIRED(二)2. Firing system In order to reasonably carry out the firing of various refractory products, the firing system of each product should be determined in advance, which includes: t... -
Jul 29, 2021HOW ARE REFRACTORY BRICKS FIRED(一)The so-called kiln installation refers to the operation process of rationally arranging and stacking bricks that meet the technical conditions of semi-finished products in the k... -
Jul 16, 2021FOUR KEY POINTS THAT AFFECT THE PERFORMANCE OF LOW CEMENT CASTABLES MUST BE K...Low-cement refractory castables are unshaped refractory materials that have been widely used in recent years, mainly including aluminum silicate, magnesia, and silicon. Its stre... -
Nov 19, 2021THE INFLUENCE OF SEVERAL COMMON MICROPOWDERS ON THE PROPERTIES OF CORUNDUM MU...As a high-temperature material, mullite has the characteristics of high softening point under load, good creep resistance and chemical resistance, low thermal expansion coeffici... -
Nov 16, 20215 CHARACTERISTICS OF ANDALUSITE IN USEAndalusite is a natural and high-quality energy-saving high-alumina refractory mineral raw material, which is mainly used in the production of refractory materials for iron and ... -
Nov 11, 2021DOES THE REFRACTORY CASTABLE FOR THE IGNITION DUCT OF THE CFB BOILER ALWAYS F...The fall of refractory castable at the ignition air duct of circulating fluidized bed boiler is a common boiler lining quality accident. This part is a refractory structure. Acc... -
Nov 05, 2021MASONRY METHOD OF REFRACTORY BRICK IN ROTARY KILN OF GARBAGE INCINERATORThe rotary kiln is an inclined steel cylinder lined with refractory materials. It is an important part of the incineration system. Various wastes are incinerated in the kiln for... -
Oct 28, 2021THE SCOPE OF APPLICATION OF FOUR COMMON WEAR-RESISTANT AND REFRACTORY PLASTICSIn the range of unshaped refractory materials, there are roughly four common types with fire-resistant and wear-resistant properties: 1. Wear-resistant and plastic Wear-resistan...