Castable Insulation
video

Castable Insulation

Castable insulation is a particular kind of castable refractory material. Castable refractory insulation is designed to have low density and thermal conductivity in order to retain heat and use less fossil fuels.
MOQ: 5 tons
Send Inquiry
Product Introduction
Description

 

Castable insulation refractory materials are critical to this energy-saving process because of their inherent low heat conductivity, as well as the benefits of ease of placement and structural strength. Due to its high permeability, insulating castable makes it easy to create dense layers that increase air tightness. The great fluidity of castable refractory insulation makes it ideal for casting construction. It can be made into a refractory and hardened without being heated. The refractoriness is comparable to that of refractory fire bricks with a similar texture.

 

Features

 

Castable insulation provides excellent insulation qualities, a high strength, a low density, and a high working temperature. Its main purpose is thermal insulation, and low density and thermal conductivity are typical design features.

 

Application

 

The steel, building, steel, and other industries all use insulating castable material. Kiln floors, soaking pit side walls, sub hearths in higher temperature applications, cooler zones, and flues/stacks can all benefit from the usage of castable insulation.

 

Physical And Chemical Indicators

 

insulation castable refractory

 

Packing And Shipping

 

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor   
By sea fumigated wooden pallet + plastic belt  + plastic film wrap.

product-750-600

Hot Tags: castable insulation, China castable insulation manufacturers, suppliers, factory, Low Cement Castable, Castable Insulation, High Strength Castable Refractories, Castable Refractories, Electric Furnace Gunning Material, Precast Block