Refractory Mortar
video

Refractory Mortar

Refractory mortar consists of refractory powder, binder and admixture. Almost all refractory raw materials can be made into powder used to prepare it.
MOQ: 5 tons
Send Inquiry
Product Introduction
Description

 

The particle size of refractory mortar varies according to the requirements of use, and its limit particle size is generally less than 1mm, and some are less than 0.5mm or finer.The material should be considered consistent with the material of refractory products of masonry. In addition to being used as a jointing material, refractory cement can also be used as a protective coating for the lining by painting or spraying.

 

Features

 

Refractory mortar has many features, such as good plasticity and convenient construction , high bonding strength, strong corrosion resistance, high refractoriness, up to 1650℃±50℃ and so on.

 

Application

 

Refractory mortar is mainly used in coke ovens, glass furnaces, blast furnace hot blast furnaces, and other industrial furnaces. The applied industries are: metallurgy, building materials, machinery, petrochemicals, glass, boilers, electric power, steel, cement, etc.

 

Physical And Chemical Indicators

 

Properties/Brand

Alumina

Clay

Insulating

MA-39

MA-38

MA-37

MA-36

MA-35

MA-34

MA-33

MA-32

MA-31

MI-1

MI-2

MI-3

Refractoriness (SK)

39

38

37

36

35

34

33

32

31

-

-

-

Chemical Composition (%)

Al2O3

80

72

62

55

45

43

40

35

30

-

-

-

SiO2

10

18

28

34

45

47

50

55

60

-

-

-

Grain Size (%) 

-1.00M

100

100

100

100

100

100

100

100

100

100

100

100

-0.074M

55

50

40

40

40

45

45

45

45

30

30

30

Bonding strength (kg/m3)

105 ℃x24hrs

15

15

15

15

15

10

10

15

15

5

5

5

1000 ℃x3hrs

15

15

20

20

20

15

15

15

15

15

6

6

1400 ℃x3hrs

30

30

35

35

35

-

-

-

-

-

-

-

Bonding Time(min)

1~3

1~3

1~3

Main Applications

Alumina & Insulating brick joint

Clay &Insulating brick joint