In Oct. 55 tons ceramic fiber blankets are packed for delivering to customer in Brazil.

A fiber blanket composed of unique crafts is called a ceramic fiber blanket. It can substantially enhance the fiber’s surface flatness, stretch strength, anti-degradation performance, and intersection. It can be installed in a variety of methods. It can be installed in Fiber Blanket Factory in a variety of ways. The two techniques that the editor put together are as follows:

1. The Fiber Blanket Factory’s set construction method for ceramic fiber blankets

(1).Ceramic fiber felt for the interior lining should be precisely cut to fit the design dimensions.

(2). There should be uniform pre-compression throughout the board for each bouquet of refractory fiber.

(3).In Fiber Blanket Factory, wear a string of fixed support plates and fixed sales, the melting should be firm, and the melting quality should be checked one by one.

(4).When fixed with a nail, compressing ceramic fiber blankets should be penetrated into the predetermined position and reached the support plate.

(5).After fixing with nails, ceramic fiber blankets should be close to the inner layer. All seams of ceramic fiber blankets should be packed closely.

2. Ceramic fiber blanket paste fixed construction method in Fiber Blanket Factory

(1).When the ceramic fiber blanket is constructed, it can be arranged by a suitable top.

(2).Before the construction of the paste method, it should be inlaid on the paste surface according to the size of each tied belt to ensure the straightness and tightness of the refractory fiber blanket.

(3).The ceramic fiber felt at the burner, the tobacco outlet and the hole should be cut into the corresponding block, and its arrangement direction should be perpendicular to the surroundings.

(4).When the steel mesh is needed, the steel mesh should be fused firmly on the furnace shell. The steel mesh should be flat, and the thickness of the steel mesh is 1-1.5 mm

(5).Paste the construction method should be carried out from top to bottom. When construction is under the bottom, do not drop the adhesive on the pasted ceramic fiber blanket.

The above are two methods for installing ceramic fiber blankets, which can be used as a reference when used. It has characteristics such as low thermal guidance, low heat capacity, excellent chemical stability and excellent stretch strength.