Alumina Ceramic Bulletproof Plate
video

Alumina Ceramic Bulletproof Plate

Alumina ceramic materials are an important part of bulletproof materials. They have high hardness and wear resistance, high compressive strength and excellent ballistic properties under high stress. Ceramics produce almost no plastic deformation when resisting the impact of a warhead, and rely on their own high strength and hardness to passivate or even break the warhead. The surface of the ceramic is crushed and absorbs the energy of the high-speed warhead in the process of forming small and hard fragments, making it bulletproof. The effect is outstanding.
Send Inquiry
Product Introduction
Products Description


Alumina ceramic Bulletproof plates are made of high-quality ceramics such as alumina, boron carbide, or silicon carbide, which have exceptional hardness, toughness, and impact resistance. These materials are formed into tiles or plates and carefully arranged in a specific pattern to create customized ballistic protection.

Alumina ceramic Bulletproof plate

 

Products Parameters

 

Alumina ceramic Bulletproof plates Parameters:
Alumina content 299%,
Density 3.88g/cm3,
Hardness>1500 (HV5),
Flexural strength>350MPA,
Impact toughness 22.2J/cm2,
Elastic modulus>320GPA. 

 

Alumina ceramic Bulletproof plate come in various sizes, shapes, and levels of protection depending on the intended use. The thickness, weight, and density of the ceramic tiles vary accordingly, with the thicker and denser ones offering higher-level protection against different types of bullets, shrapnel, and fragments.

 

Products Advantages

 

1. Lightweight: Ceramic materials are much lighter than steel or other metals, making them ideal for situations where mobility and flexibility are required.

2. High impact resistance: The ceramic tiles have excellent resistance to impact, which means they can withstand multiple hits without breaking or cracking.

3. High hardness: The hardness of ceramic materials is comparable to that of diamond, which means they can withstand high-velocity impacts from high-powered rifles.

4. Customizable:  Alumina ceramic Bulletproof plate can be customized to fit specific body armor, vehicles, or structures, providing maximum protection.

5.trong bulletproof ability: The main component of alumina ceramics is α-alumina, which has stable chemical properties and extremely high hardness. It will not reduce its performance under high temperature, oxidation, etc., and can crush and absorb warheads with extremely high hardness. Energy to achieve bulletproof purposes, the bulletproof level reaches American standard level 4, which can meet most bulletproof requirements.

6.Cheap price: Alumina bulletproof ceramics are slightly more expensive than metal bulletproof materials, but their performance far exceeds that of metal materials. Compared with silicon carbide and boron carbide, its price is very cheap. Taking into account the cost and cost of various materials, Properties such as rigidity and strength, and keeping the cost as low as possible while ensuring that the bulletproof performance meets the specified requirements, are the important reasons why alumina bulletproof ceramics are so popular.

 

Products Application

 

1. Personal protection: Alumina ceramic Bulletproof plates are incorporated into personal protective gear such as vests, helmets, and shields to provide reliable defense against bullets, fragments, and shrapnel.

2. Vehicle armor: Ceramic plates are used to reinforce the armor of vehicles such as tanks, armored cars, and helicopters, providing enhanced protection against ballistic threats.

3. Infrastructure protection: Ceramic armor Bulletproof plates are used to reinforce critical infrastructure such as embassies, government buildings, and nuclear facilities, to protect against potential terrorist attacks.

ceramic bulletproof plate

 

 

Products Precautions for use

 

Avoid excessive impact: Although Alumina ceramic Bulletproof plate have high impact resistance, excessive impact may still cause them to break or fail, so excessive impact should be avoided when using them.

Avoid high temperatures: Bulletproof ceramic sheets may deform or crack at high temperatures, so high-temperature environments should be avoided during storage and use.

Pay attention to protection: When carrying or storing bulletproof ceramic sheets, be careful to avoid friction with sharp objects or other hard objects to avoid damaging the surface of the ceramic sheets.

 

DescTechnical Parameters:
Almina content 299%,
Density 3.88g/cm3,
Hardness>1500 (HV5),
Flexural strength>350MPA,
Impact toughness 22.2J/cm2,
Elastic modulus>320GPA.ription

 