Bulletproof alumina insert plate have high specific stiffness, high specific strength and chemical inertness in many environments. Compared with metal, Bulletproof Vest Plate will plastically deform and absorb energy when resisting the impact of the bullet, but it hardly generates plastic deformation, and due to its high strength and high hardness, the bullet can be passivated or even broken, and the ceramic surface is crushed at the same time in the formation of small particles. And the hard fragment area absorbed the energy of the high-speed warhead.

 

Features

 

Bulletproof alumina insert plate has the character of high conformity to human body curve, high and good quality content of raw materials, strong protective performances and strong energy absorption ability.

 

Application

 

Bulletproof alumina insert plate is widely used in body armor, protective armor for vehicles and aircraft and other equipment.

 

Physical And Chemical Indicators

 

Product Category Ⅰ Ⅱ
Material 84.2%Alumina+14.1%Zirconia 99% Alumina
Protection level NIJⅢ 、NIJⅣ NIJⅢ 、NIJⅣ
Size 300*250mm 300*250mm
Bending strength 457 Mpa 419 Mpa
Elastic Modulus 327 Gpa  315Gpa
Bulk density 4.10g/cm3 3.97g/cm3
Compressive strength 1908 Mpa 1897 Mpa
Rockwell hardness 90.7 HRA 89.3HRA

 

Packing And Shipping

 

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By packing it with a small bubble bag and put it in the box

 

product-750-521

Hot Tags: bulletproof alumina insert plate, China bulletproof alumina insert plate manufacturers, suppliers, factory, Bulletproof Alumina Insert Plate, High Alumina Ceramic Material, Alumina Ceramic Honeycomb Ceramic, Alumina Ceramic Roller, Alumina Wear Resistant Ceramic, Ceramic Ball

Send Inquiry

whatsapp

Phone

E-mail

Inquiry