Alumina Lining Brick
video

Alumina Lining Brick

Alumina lining brick is a product used for wear-resistant lining of ball mills, which is widely used in ceramics, cement, paint, pigment, chemical, pharmaceutical, coating and other industries.
MOQ:5 tons
Send Inquiry
Product Introduction
Description

 


Alumina lining brick is a high purity refractory material, usually made from alumina and other additives through molding, drying and sintering processes. It has excellent high temperature performance and chemical stability, can be used at high temperature for a long time without deformation or fracture.
According to the shape, it is divided into: rectangular brick, trapezoidal brick and special-shaped brick.
Also known as ceramic lining brick, high alumina lining refractory brick, alumina lining brick, 92 porcelain lining, ceramic lining, ball mill lining, high alumina lining, microcrystalline wear-resistant alumina lining  fire brick, etc.

 

Features

 

1. It is high-quality alumina with high purity, which greatly reduces the pollution of grinding materials.
2. Good wear resistance, which is 266 times that of manganese steel, effectively prolonging the service life of the equipment
3. The slurry is finely ground when matched with high-aluminum balls; it has the characteristics of corrosion resistance, high density, and high mechanical strength.

 

Application

 

Alumina lining brick can be used for grinding glazes and ceramic tiles. The product has the characteristics of high hardness, high density, low abrasion, good regularity, corrosion resistance, etc. It is used for wear-resistant lining of ball mills, and is widely used in ceramics, cement, paint, pigments, chemicals, medicine, coatings, inorganic mineral powders, etc. Industry, can effectively improve grinding efficiency, reduce grinding costs, and reduce product pollution.

 

Physical And Chemical Indicators

Properties

ALB-92

ALB-92S

ALB-95

 Al2O3(%)

≥92

≥92

≥95

Bulk density(g/cm3)

≥3.65

≥3.68

≥3.68

Wear Loss(%)

≤0.01

≤0.008

≤0.01

Hardness(Mohs)

9

9

9

Water Absorption(%)

≤0.01

≤0.01

≤0.01

 Color

white

white

white

Size

 

Length(mm)

 (W1)

Width (mm)

 (W2)

Width (mm)

 (H)

Height (mm)

End Flat Brick

150

50

50

40/50/60/

70/77/90

Circle Brick

150

50

45

 

 Half End Flat Brick

75

50

50

 

Half Circle Brick

75

50

45

 

 Flake Brick

150

25

22.5

 

Size can be customized

Hot Tags: alumina lining brick, China alumina lining brick manufacturers, suppliers, factory, Alumina Wear Resistant Ceramic, Ceramic Ball, High Alumina Ceramic Material, Plate Ceramic Wear Lining Tile, Alumina Ceramic Roller, Alumina Ceramic Honeycomb Ceramic

Send Inquiry