Alumina Ceramic Lining Plate And Piece
video

Alumina Ceramic Lining Plate And Piece

Alumina Ceramic Lining Plate And Piece is a high-temperature refractory material made of alumina (Al2O3) as the main raw material. It has excellent wear resistance, corrosion resistance and high temperature resistance, and is suitable for high temperature equipment and furnace linings in various industrial fields.
Send Inquiry
Product Introduction
Products Description

 

Alumina Ceramic Lining Plate And Piece is an ideal high-temperature refractory material with excellent refractory performance, wear resistance and corrosion resistance, and is widely used in high-temperature equipment and furnace linings in metallurgy, glass, chemical, electric power and other industries. It can protect equipment from high temperature and corrosion damage, prolong the service life of equipment, and improve production efficiency and safety.

 

Products Features

 

Fire resistance: Alumina has excellent high temperature resistance and can withstand temperatures as high as 1600°C. This makes alumina ceramic linings an ideal choice for high temperature processes such as metallurgy, glass, chemical and ceramic industries.

Wear resistance: Alumina Ceramic Lining Plate And Piece has excellent wear resistance and can withstand the impact of mechanical wear and abrasives. This makes it widely used in the lining of coal mills, ball mills, mortar mixers and other equipment.

Corrosion resistance: Alumina ceramic lining has good chemical stability and can resist the erosion of acid and alkali solutions, corrosive gases and molten metals. Therefore, it is often used in pickling tanks, electrolytic tanks in the chemical industry, and furnaces and containers in the metallurgical industry.

Insulation performance: Since alumina ceramic liners have low thermal and electrical conductivity, they can provide good insulation performance. This makes them widely used in the electronics industry and high temperature insulation equipment.

Variety of shapes: Alumina Ceramic Lining Plate And Piece can be made into different shapes and sizes according to specific application requirements. Common shapes include brick, tile, pipe, lumber, and custom pieces. This flexibility allows alumina ceramic liners to adapt to a variety of different equipment shapes and sizes.

 

aluminum lining plate and piece

Application

 

Metallurgical industry: Alumina ceramic linings are widely used in the lining of high-temperature furnaces, smelting furnaces, converters and ladles in the metallurgical industry, which can resist high temperature and corrosive gases.
Glass industry: It is widely used in equipment such as glass furnaces, baths and crucibles in the glass industry, and can withstand the special environment of high temperature and glass corrosion.
Chemical industry: Alumina Ceramic Lining Plate And Piece is often used in reaction kettles, steam pipelines, pickling tanks and other equipment in the chemical industry, which can resist the corrosion of acid and alkali solutions.
Power industry: It is used as the inner lining of boilers and power equipment in the power industry, which can withstand the effects of high temperature and thermal shock.

 

aluminum ceramic lining plate

                                                                                       Production plant

 

Physical and Chemical Indicators

 

Properties&Brand 92 Series 95 Series 97 Series 99 Series
Bulk Density (g/cm3) ≥ 3.63 ≥ 3.68 ≥ 3.73 ≥ 3.83
Moisture Content (%) ≤0.02 ≤0.02 ≤0.02 ≤0.02
Fracture Toughness (%) 40 42 44 48
Al2O3 Content (%) ≥92 ≥95 ≥97 ≥99
Bending Strength 255 275 285 300

 

Hot Tags: Alumina Ceramic Lining Plate And Piece, China Alumina Ceramic Lining Plate And Piece manufacturers, suppliers, factory, Ceramic Lining Plate, Alumina Wear Resistant Ceramic, High Alumina Ceramic Material, Alumina Honeycomb Ceramics, Alumina Ceramic Roller, Alumina Lining Brick