Alumina Mosaic Tiles
video

Alumina Mosaic Tiles

Alumina Mosaic Tiles are the first choice for industrial wear-resistant, impact-resistant and corrosion-resistant materials. Common squares and hexagons.
MOQ<5tons
Send Inquiry
Product Introduction
Products Description

 

 

The main function of the Alumina Mosaic Tiles is to effectively resist the impact of the material on the pipe wall, the corrosion of chemical substances and the thermal shock of the material, and reduce the wear and tear on equipment components, thus greatly reducing the cost of frequent maintenance. , extend the service life of the equipment.

 

 

 

alumina mosaic tile-2

 

Products Parameters

 

Brand
Properties

AMT-92

AMT-95

Al2O3(%)

≥92

≥95

Bulk density(g/cm3)

≥3.6

≥3.65

Wear Loss(%)

≤0.01

≤0.01

Hardness(Mohs)

9

9

Color

white

white

Size

Length(mm)

Width (mm)

Thickness (mm)

Square Shape

10-24

10-24

3-20

Hexagon Shape

12-20

12-20

3-15

Size can be customized

 

Products  features

 

1. High hardness: The Alumina Mosaic Tiles hardness can reach Mohs hardness level nine, second only to diamond and far exceeding the wear resistance of wear-resistant steel and stainless steel.
2. Good wear resistance: the wear resistance is equivalent to 266 times that of manganese steel and 171.5 times that of high chromium cast iron. Under the same working conditions, the service life of the equipment can be extended by at least ten times.
3. Light weight: The density is 3.6g/cm3, which is only half of steel, which can greatly reduce the equipment load.
4. Firm bonding and good heat resistance: The wear-resistant ceramic sheets are pasted on the inner wall of the equipment with heat-resistant strong glue. It can operate for a long time at 350℃ without aging.

 

Products Application 

 

Alumina Mosaic Tiles used in coal conveying, material conveying systems, pulverizing systems, ash discharge, dust removal systems and other mechanical equipment with high wear in enterprises such as thermal power, steel, smelting, machinery, coal, mining, chemical industry, cement, ports and terminals.

 