Ceramic Fiber Tape
video

Ceramic Fiber Tape

Ceramic fiber tape is a high-temperature resistant textile processed by textile technology using ceramic fiber cotton as the main material, alkali-free glass filaments or high-temperature-resistant stainless steel alloy wire as reinforcing materials.
MOQ<5TONS
Send Inquiry
Product Introduction
Products Description

 

Ceramic fiber tapes, also known as ceramic tapes, aluminum silicate fiber tapes, and aluminum silicate tapes, have properties such as high temperature resistance, open flame non-combustibility, and thermal insulation. They can be used as insulation and friction materials for various thermal equipment and heat transfer systems.

high purity alumina-silica fiber tape exhibits remarkable thermal stability and resistance to thermal shock.The manufacturing process involves the precise blending of ceramic fibers and other additives to achieve the desired composition. This mixture is then processed using advanced weaving technology, resulting in a flexible and durable tape that can withstand temperatures exceeding conventional insulating materials.

 

Brand

Properties

Bio-Soluble  fiber tape

Ceramic fiber tape

GF-Rope/Cloth/Tape/Yarn

SS-Rope/Cloth/Tape/Yarn

GF-Rope/Cloth/Tape/Yarn

SS-Rope/Cloth/Tape/Yarn

Specification Temp. (℃)

1260

Working Temp. (℃)

500-600

1100

500-600

1100

Bulk Density (kg/m3)

500

Organic matter

15

Moisture Content(%)

1


ChemicalComposition

SiO2

55-65

51

CaO

23-35

--

MgO

5-10

--

Al2O3

--

45

Fe2O3

--

0.8

Reinforced material

Glass Filament

stainless steel 304

Glass Filament

Stainless steel 304

 

 

Products Features

 

High-Temperature Resistance: Ceramic fiber tape is engineered to withstand temperatures up to 2300°F (1260°C), making it an ideal choice for applications in furnaces, kilns, and other high-heat environments.
Flexibility and Versatility: The tape's pliable nature allows for easy wrapping around complex shapes and structures, providing a seamless insulation solution.
Low Thermal Conductivity: Its low thermal conductivity ensures efficient insulation, preventing heat loss and contributing to energy conservation.
Chemical Stability: Resistant to most chemicals, the tape maintains its structural integrity in corrosive environments, adding to its longevity.

Ceramic fiber tapes are generally sized in terms of width and thickness. Common width specifications are 10mm, 20mm, 30mm, 40mm, etc., and thickness specifications are 1mm, 2mm, 3mm, 5mm, etc. At the same time, customized sizes can also be made according to different uses and needs. When using ceramic fibre tapes, it is necessary to select the appropriate size according to the specific situation to ensure the use effect. 

 

Products Advantage

 

ceramic fibre tape

 

(1) Ceramic fiber tape continuous use temperature can reach 1050℃ (stainless steel wire reinforced) , or 650℃ (glass wire reinforced), the former can reach 1260℃ in a short time.
(2) It has good resistance to acid and alkali corrosion and corrosion resistance to molten metals such as aluminum and zinc.
(3) Good high-temperature strength and thermal insulation performance .
(4) Ceramic fiber cloth, tape, packing and other series of products using alkali-free glass fiber as reinforcing materials have higher electrical insulation and high-temperature electrical insulation than glass fiber.
(5) Non-toxic, harmless and odorless.

Note: Ceramic fiber textiles contain about 15% organic fibers. When used for the first time and the temperature rises, the organic fibers in the product will gradually carbonize and turn black, and smoke will appear. There may be flames in some places. occurs, this is a normal phenomenon and does not affect use. As the temperature continues to rise, the product will gradually turn white, the organic fibers have been completely carbonized, and the product is completely made of high-temperature-resistant inorganic materials such as ceramic fibers.

 

Products Usage

 

Ceramic fiber tape is used in many different industries where insulation against high temperatures is crucial.
insulation of high-temperature pipelines, containers, and different types of kilns;
high temperature furnace door sensitive curtains, flange seals, valves, fire doors, and fire shutter materials;
fireproof cable wrapping materials, insulation for engines and instruments, and high-temperature fireproof materials;
Material for flue lining, expansion joint filler at high temperatures, and thermal insulation covering;
High temperature resistant labor protection goods, fireproof clothing, high temperature filtration, sound absorption and other asbestos substitution uses.

application

 

Hot Tags: ceramic fiber tape, China ceramic fiber tape manufacturers, suppliers, factory, ceramic fiber gasket material, Rock Wool board, ceramic fiber gasket temperature, Aerogel Refractory Blanket, Vermiculite Refractory Board, ceramic fiber gasket paper

Send Inquiry

whatsapp

Phone

E-mail

Inquiry