650℃ Calcium Silicate Board
Products Description
A new form of white, hard insulation material 650℃ calcium silicate board : it is lightweight, strong, has low thermal conductivity, can withstand high temperatures, resists corrosion, and is cutting-resistant. Refractoriness is 650C, and it is widely applicable in petrochemical, power plant, building, and vessel fields. Generally speaking, the thickness is between 25 and 120 mm, and the density is between 250 and 300 kg/m3.
Products Parameters
650℃ calcium silicate board parameters
1.Temperature Resistance: Up to 650℃ (or higher in some variants)
2.Density: Typically ranges from 200 to 1000 kg/m³
3.Thickness: Varies from a few millimeters to several centimeters
4.Dimensions: Customizable based on application needs
5.Compressive Strength: Generally high, ensuring stability under pressure

650℃ Calcium Silicate Board Production Process
Raw Material Preparation: Calcium silicate boards are typically made from silica sand, lime, and reinforcing fibers.
Mixing & Forming: The raw materials are mixed and formed into boards using a combination of pressing, extrusion, or molding techniques.
Curing & Setting: The formed boards undergo a curing process, where heat and pressure are applied to facilitate the setting of the materials.
Cutting & Finishing: After curing, the boards are cut into desired sizes and shapes and undergo finishing processes if required.

650℃ Calcium Silicate Board Features
High Temperature Resistance: Ideal for applications requiring insulation or protection against high heat.
Excellent Thermal Insulation: Offers effective insulation properties, minimizing heat transfer.
Low Thermal Conductivity: Helps conserve energy and maintain stable temperatures.
Chemical Resistance: Resistant to many chemicals, making it suitable for harsh environments.
Durable & Strong: Provides structural stability and withstands mechanical stress.
650℃ Calcium Silicate Board Application
Industrial Furnaces & Kilns: Used as linings to insulate and protect against high temperatures.
Petrochemical & Power Plants: Applied in areas needing thermal insulation and fire protection.
Oven & Dryer Insulation: Utilized in commercial and industrial baking ovens, dryers, etc.
Building Construction: Used for fire-resistant partitions, ceilings, and wall linings in construction.

Hot Tags: 650℃ calcium silicate board, China 650℃ calcium silicate board manufacturers, suppliers, factory, Insulation Aerogel Blanket, Ceramic Fiber Rope, Corudum Mullite Cordierite brick, Ceramic Fiber Cotton, Calcium Silicate Board, Rockwool Insulation Slabs