Insulation Alumina Silicate Needles Ceramic Fiber Blanket
video

Insulation Alumina Silicate Needles Ceramic Fiber Blanket

Insulation Alumina silicate Needles Ceramic Fiber Blanket is a high-temperature resistant material composed of high purity alumina, silica, and zirconia fibers. This lightweight, flexible ceramic fiber blanket provides excellent thermal insulation qualities, it effcient at restricting heat fow, while maintaining other key material properties such as low shrinkage and good mechanical durability.
Send Inquiry
Product Introduction
Products Description

 

Insulation Alumina silicate Needles Ceramic Fiber Blanket is a high-quality insulation material that is widely used in various industries due to its excellent performance and durability. Made from high-purity alumina-silica ceramic fibers, this product possesses exceptional thermal stability and heat resistance, making it suitable for use in environments with temperatures up to 1430℃.
it has superior thermal insulation properties. It has a low thermal conductivity of just 0.09 W/mK, making it an excellent choice for insulation applications.

It also has a high tensile strength of up to 4.5 Mpa, making it durable and long-lasting.

 

 Features and Benefits

The Insulation Alumina silicate Needles Ceramic Fiber Blanket have excellent heat resistance, low thermal conductivity, and high tensile strength.
It is a versatile thermal insulation material that can be used in numerous applications, from boiler lining to furnace insulation.
Its excellent thermal insulation properties can help to prevent heat loss and reduce energy costs.
The material is also resistant to thermal shock, chemical attack, and moisture, ensuring that it can withstand the harshest of environments.


Insulation Alumina silicate Needles Ceramic Fiber Blanket Benefits
Improved energy efficiency and fuel savings
Reducing CO2_emissions
lmprove operational costs and overall performance Design
flexibility and variety of application opportunities

 

ceramic fiber blanket


 

Products production process

The production of Insulation Alumina silicate Needles Ceramic Fiber Blanket

First,the selection and blending of high purity raw materials.
second ,The blended materials are then sent to a furnace where the temperature is gradually increased to a level that allows the fibers to fuse together.
third,The resulting material is then formed into rolls or blankets of various thicknesses and densities.

Insulation Alumina silica Needles Ceramic Fiber Blanket production

 

Products Application

Insulation Alumina silicate Needles Ceramic Fiber Blanket application
It can be attached directly to the inner wall of the boiler lining,kiln linings,furnace insulation, or they can be fixed to the steel structure with metal clips. This blanket-like material is soft and wear-resistant, and is very convenient in terms of installation and maintenance, making the lining of the kiln more optimized and convenient.
Its versatility and excellent thermal insulation properties make it a popular choice for various industries, including metalworking, power generation, and petrochemical.

 

application

 

Hot Tags: Insulation Alumina Silicate Needles Ceramic Fiber Blanket, China Insulation Alumina Silicate Needles Ceramic Fiber Blanket manufacturers, suppliers, factory, Chrome Ceramic Fiber Blanket for furnace lnsulation, Zirconia Blanket, Rockwool Board, Microporous Board, Stainless Steel Anchor, Aerogel Refractory Blanket