In life, there are many refractory materials for alkaline resistance, but according to the degree of corrosion of different temperatures, the refractory water -resistant pouring materials or anti -alkali resistance bricks are selected according to the degree of corrosion of different temperatures. Bricks, alkali resistance, lightweight alkali and bricks.

Magnesium, magnesium bricks, magnesium aluminum spine -spine tiles, magnesium chromium bricks, magnesium iron spine -tianli bricks, Mgo Spinel Brick, phosphate bricks, phosphate composite bricks, and alkaline resistance refractory resistance resistance The pouring materials are resistant to alkaline -resistant pouring materials, anti -skin pouring materials, rigida molt stone pouring, magnesium aluminum spikes, chromium rigid jade pouring materials, and magnesium prefabricated parts. The alkaline -resistant -resistant kiln lining with alkali resistance can make the atmosphere of the firing material of the kiln lining. Under the same circumstances, the product has good activity, and different brick shapes are designed according to the size of different kiln linings.

Mgo Spinel Brick is a series of crystals with the same image structure as magnesium aluminum spinel MA. Magnesium aluminum spinels belong to cubic products. Magnesium chromium spinel rotation is an equivalent crystal mineral, hardness of 5.5, relative density 4.43, refractive index n = 2.00 but no magnetic, magnesium aluminum spine -spine tiles are natural magnesium materials such as magnesium stone, light -roasted magnesium powder As the material with chromium iron ore, cooperate in accordance with the planning requirements, fine grinding, ball pressing, burning, or melt obtained by the melting of magnesium chromium spinel as the main ingredient, my country’s black gold industry specification YB/T132-1997 regulations The skill conditions of Mgo Spinel Brick.

When making sintering Mgo Spinel Brick, the ratio of the planning is forced according to the planning requirements. It is made after the cooperation melting. Mgo Spinel Brick crystals, tissue tightness, low pores, and high degree of direct combination. Therefore, the melting casting is an excellent corrosion resistance in combination with magnesium chromium bricks, and is widely used for very stringent corrosion. However, the heating shocks of the magnesium chromium brick are directly combined with magnesium chromium bricks from magnesium and iron ore.

Mgo Spinel Brick is a kind of refractory material with high melting point, small thermal expansion coefficient, low thermal conductivity, good thermal shock stability, and strong resistance to erosion. Magnesium aluminum spinel bricks are classified as a shafts of the shafts, and high -purity Mgo Spinel Brick is colorless.