The tertiary air duct of cement rotary kiln is an important part. Its main function is to connect the hot air duct between the cooler and the rotary kiln system. The working environment of the tertiary air duct is very harsh, including Y-shaped parts, elbows and closing valves. The damage is serious and the usage conditions are the most severe. The main cause of damage to the refractories materials here is the erosion, abrasion and corrosion of alkali, sulfur and chlorine caused by high-temperature gases carrying a large amount of dust and containing alkali, sulfur and chlorine. The refractory materials are prone to wear, looseness and peeling.
Refractory material for tertiary air ducts include high-strength alkali-resistant bricks, high-strength alkali-resistant castables, wear-resistant castables, wear-resistant castable prefabricated parts, calcium silicate boards, diatomaceous earth bricks and lightweight castables.

1. High strength alkali resistant bricks
There are four main types of alkali-resistant bricks used in cement rotary kilns, namely ordinary type, high-strength type, vault type and heat-insulating type. Among them, the alkali-resistant bricks used in the tertiary air ducts are high-strength alkali-resistant bricks, whose main feature is strong resistance to alkali erosion. However, with the continuous development of the cement industry, high-strength alkali-resistant bricks have gradually been replaced by silica-molybdenum bricks.
2. High strength alkali resistant castable
High-strength alkali-resistant castables have similar properties to high-strength alkali-resistant bricks. They both have super alkali corrosion resistance and can resist the erosion of alkali metal oxides (such as K2O and Na2O) at medium and high temperatures. The castable is mainly a mixture of alkali-resistant refractory aggregates and powders, binders and admixtures.
The alkali-resistant mechanism of alkali-resistant refractory materials castables is that they react with alkali metal oxides at high temperatures to form a high-viscosity liquid phase, forming a glaze-like protective layer to prevent the penetration and erosion of alkali metal melts.
3. Wear resistant castables and wear resistant castable prefabricated parts
Wear-resistant castables refer to refractory castables with high wear resistance. The smaller the wear amount of wear-resistant castables when measured, the better the wear resistance of the castables. The wear-resistant performance of wear-resistant castables mainly comes from the use of refractory raw materials such as fused corundum, sintered corundum, fused zirconium corundum, silicon carbide, and silicon nitride. In addition, in order to improve the stiffness and wear resistance of the material, heat-resistant steel fibers are generally added.
Wear-resistant refractory materials castable prefabricated parts are products that are prefabricated with alkali-resistant castables in production companies according to the parts to be used, and then transported to the construction site for direct assembly. Compared with wear-resistant castables, the performance of wear-resistant castable prefabricated parts is equivalent to, or even higher than, castables. The biggest advantage of wear-resistant castable prefabricated parts is that they are easy to construct, shorten the construction period, and save labor costs.
4. Calcium silicate board
Calcium silicate board is an insulating and refractory product made of diatomite and lime as the main raw materials and added with reinforcing fibers. It is also called calcium silicate board. Calcium silicate board can be sawed or nailed, and can be made into shapes such as boards, blocks or sleeves.
5. Other materials
In addition to the above four types, materials commonly used in tertiary air ducts include diatomite bricks, lightweight castables, silica molybdenum bricks and other materials. In actual masonry construction needs, it is necessary to meet the actual work requirements of three air ducts, select appropriate refractory materials, and cooperate with strict construction control and correct oven methods to create a long-life cement rotary kiln production system.