What Are The Matters That Must Be Paid Attention To in Refractory And Plastic Difficulties?

The construction method of refractory can be used for plastic and refractory pouring materials. It can take more than 16 hours before plastic construction for more than 16 hours to carry out construction.

 

The description of the refractory can be plastic before construction

Because the manufacturers do not understand a lot of materials, if it is a professional construction team, the construction is not a problem, but the use of the manufacturer with the employees of the unit or the temporary worker to be temporarily found for construction.

The refractory -resistant plastic material cannot be less than 16 hours before construction. There are two ways to produce the production of plastic manufacturers. One is to add one -third or a quarter of a binding agent directly in the manufacturer. The material is directly completed during transportation, and the remaining binding agents can be directly constructed when they are used.Before using refractory plastic, the material should be thoroughly stirred to ensure that the components are evenly mixed. The mixed plastic should be stored in a dry and well-ventilated place to avoid moisture and pollution. Before trapping materials, the fixed or masonry surface should be thoroughly cleaned to ensure that it is free of dust, oil and other impurities. A clean surface aids the adhesion between the refractory plastic and the base material.

 

news-640-407

 

Matters of plastic attention on the trapped material

Some of the plastic can not be added during the production process, and it is necessary to use the on -site on -site to build it. However, there are some manufacturers without construction experience. Even if they see the construction description step and the combined agent, it is still unsuccessful. The refractory resistance can be used to solidify first, or it cannot be used when it is trapped in construction.

It should be noted that when the combination agent is added, only one -third of the phosphoric acid solution of the barrel must be added. Hold it into a group with your hands and let go of your hand into a scattered shape. Other additives (such as high aluminum cement in a small bag in the bag) cannot be added. The additives can only be used for more than 16 hours, that is, add stirring during use, and then add the remaining phosphoric acid solution to use.


If it is not possible to add high aluminum cement when it is difficult, the material will be solidified after adding it. The high aluminum cement can only be stirred when the refractory resistance is started construction. Add the remaining phosphoric acid solution to make any shapes for construction.